Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.481 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.123 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 191.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 38.2 |
C (mp-48) | <1 0 1> | <0 0 1> | 305.8 |
C (mp-48) | <1 1 0> | <0 0 1> | 267.6 |
C (mp-48) | <1 1 1> | <0 0 1> | 305.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 329.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 191.1 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 267.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 305.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 191.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 89.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 114.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 274.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 200.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 179.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 344.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 305.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 267.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 89.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 191.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 191.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 89.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 97.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 267.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 305.8 |
InP (mp-20351) | <1 1 0> | <0 1 1> | 200.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 152.9 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 191.1 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 269.1 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 0> | 219.5 |
CdWO4 (mp-19387) | <1 1 1> | <0 1 1> | 200.6 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 179.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 267.6 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 191.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 267.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 152.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 344.0 |
BN (mp-984) | <1 0 0> | <1 0 1> | 97.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 344.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 267.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 229.3 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 133.7 |
Al (mp-134) | <1 0 0> | <1 0 1> | 97.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 267.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 305.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 344.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 219.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 329.2 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 179.4 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 274.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.42950 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.29402 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.57178 |
Piezoelectric Modulus ‖eij‖max0.57178 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
5.38 | 0.00 | 0.00 |
0.00 | 5.33 | 0.00 |
0.00 | 0.00 | 5.40 |
Dielectric Tensor εij (total) |
||
---|---|---|
15.50 | 0.00 | 0.00 |
0.00 | 14.50 | 0.00 |
0.00 | 0.00 | 16.79 |
Polycrystalline dielectric constant
εpoly∞
5.37
|
Polycrystalline dielectric constant
εpoly
15.60
|
Refractive Index n2.32 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaGa4O7 (mp-769971) | 0.6090 | 0.000 | 3 |
SrAl4O7 (mp-3788) | 0.6171 | 0.000 | 3 |
NaP4N7 (mp-29598) | 0.5948 | 0.000 | 3 |
BaAl4O7 (mp-1019534) | 0.4686 | 0.001 | 3 |
CeSi3N5 (mp-29466) | 0.0530 | 0.003 | 3 |
Li2FeSi3O8 (mp-767149) | 0.6163 | 0.075 | 4 |
KLiSi2O5 (mp-558102) | 0.5087 | 0.000 | 4 |
Li2MnSi3O8 (mp-761653) | 0.5912 | 0.076 | 4 |
RbLi2Be2F7 (mp-560518) | 0.5952 | 0.000 | 4 |
Na2Zn5(PO4)4 (mp-560934) | 0.6200 | 0.000 | 4 |
CeSe2 (mp-1080359) | 0.7071 | 0.507 | 2 |
KLiZnP2O7 (mp-554164) | 0.6853 | 0.000 | 5 |
SrAl2SiN2O3 (mp-554390) | 0.2281 | 0.003 | 5 |
LaAl2Si5N9O (mp-677482) | 0.7385 | 0.151 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.7437 | 0.003 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Si N |
Final Energy/Atom-8.2552 eV |
Corrected Energy-297.1886 eV
-297.1886 eV = -297.1886 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)