material

ZrBeSi

ID:

mp-10200

DOI:

10.17188/1186811


Tags: Zirconium beryllium silicide (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.747 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.84 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 76123 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ge (mp-32) <1 1 1> <0 0 1> 0.000 230.1
Al (mp-134) <1 1 1> <0 0 1> 0.000 84.8
GaP (mp-2490) <1 1 1> <0 0 1> 0.000 157.5
LaF3 (mp-905) <1 0 1> <1 1 0> 0.006 140.8
CdSe (mp-2691) <1 1 0> <1 0 1> 0.008 326.5
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.014 157.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.015 84.8
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.017 48.5
GaAs (mp-2534) <1 1 1> <0 0 1> 0.018 230.1
GaSb (mp-1156) <1 1 0> <1 0 1> 0.022 326.5
Ni (mp-23) <1 1 1> <0 0 1> 0.026 84.8
ZnTe (mp-2176) <1 1 0> <1 0 1> 0.027 326.5
InSb (mp-20012) <1 1 1> <0 0 1> 0.036 230.1
InAs (mp-20305) <1 1 0> <1 0 1> 0.038 326.5
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.040 140.8
Cu (mp-30) <1 1 1> <0 0 1> 0.041 157.5
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.045 230.1
PbSe (mp-2201) <1 1 0> <1 0 1> 0.048 326.5
CdTe (mp-406) <1 1 1> <0 0 1> 0.051 230.1
GaN (mp-804) <1 1 1> <1 0 0> 0.054 243.9
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.057 230.1
NdGaO3 (mp-3196) <0 0 1> <1 0 0> 0.057 243.9
SiC (mp-11714) <1 0 1> <1 0 1> 0.087 356.2
SiC (mp-8062) <1 1 1> <0 0 1> 0.092 230.1
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.092 193.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.098 109.0
AlN (mp-661) <0 0 1> <0 0 1> 0.098 109.0
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.104 254.4
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.105 267.1
SiC (mp-11714) <0 0 1> <0 0 1> 0.109 109.0
BN (mp-984) <1 1 1> <0 0 1> 0.109 205.9
SrTiO3 (mp-4651) <1 0 0> <1 0 1> 0.110 89.0
SrTiO3 (mp-4651) <1 1 1> <1 1 0> 0.113 140.8
MgAl2O4 (mp-3536) <1 0 0> <1 0 1> 0.115 267.1
YVO4 (mp-19133) <1 0 1> <1 1 0> 0.119 140.8
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.128 109.0
Si (mp-149) <1 1 1> <0 0 1> 0.144 157.5
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.146 230.1
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.147 121.1
Ga2O3 (mp-886) <1 0 0> <1 1 1> 0.150 145.4
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.154 157.5
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.156 267.1
GaN (mp-804) <0 0 1> <0 0 1> 0.161 36.3
Al2O3 (mp-1143) <1 0 1> <1 0 1> 0.162 267.1
Cu (mp-30) <1 0 0> <1 0 1> 0.169 118.7
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.174 193.8
C (mp-48) <1 0 0> <0 0 1> 0.177 230.1
LaF3 (mp-905) <1 0 0> <1 0 0> 0.189 54.2
BN (mp-984) <0 0 1> <0 0 1> 0.200 48.5
Al2O3 (mp-1143) <1 0 0> <1 1 0> 0.201 187.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
299 68 71 0 0 0
68 299 71 0 0 0
71 71 234 0 0 0
0 0 0 132 0 0
0 0 0 0 132 0
0 0 0 0 0 116
Compliance Tensor Sij (10-12Pa-1)
3.7 -0.6 -0.9 0 0 0
-0.6 3.7 -0.9 0 0 0
-0.9 -0.9 4.8 0 0 0
0 0 0 7.6 0 0
0 0 0 0 7.6 0
0 0 0 0 0 8.6
Shear Modulus GV
117 GPa
Bulk Modulus KV
139 GPa
Shear Modulus GR
115 GPa
Bulk Modulus KR
137 GPa
Shear Modulus GVRH
116 GPa
Bulk Modulus KVRH
138 GPa
Elastic Anisotropy
0.11
Poisson's Ratio
0.17

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CeNiAs (mp-1061766) 0.0086 0.000 3
CaZnSi (mp-16266) 0.0074 0.000 3
BaSnHg (mp-11819) 0.0005 0.000 3
SmNiAs (mp-16734) 0.0190 0.000 3
BaLiP (mp-13277) 0.0120 0.000 3
YSi2 (mp-2568) 0.0157 0.041 2
HoGa2 (mp-1256) 0.0119 0.000 2
TbSi2 (mp-1535) 0.0050 0.023 2
ErGa2 (mp-2422) 0.0001 0.000 2
DyGa2 (mp-20064) 0.0146 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Be_sv Si
Final Energy/Atom
-6.6503 eV
Corrected Energy
-39.9020 eV
-39.9020 eV = -39.9020 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 76123
Submitted by
User remarks:
  • Zirconium beryllium silicide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)