Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.208 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2SiO3 + Ca2SiO4 |
Band Gap4.738 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6122 [178] |
HallP 61 2 (0 0 1) |
Point Group622 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 368.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 138.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 345.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 115.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 138.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 253.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 161.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 69.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 299.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 207.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 276.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 276.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 184.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 276.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 161.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 161.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 69.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 207.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 276.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 230.3 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 276.4 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 368.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 161.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 69.1 |
C (mp-48) | <1 0 1> | <0 0 1> | 253.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 23.0 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 322.4 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 299.4 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 276.4 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 184.3 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 322.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 299.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 161.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 207.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 368.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 161.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 276.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 69.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 23.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 207.3 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 115.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 207.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 115.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 276.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 69.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 207.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 276.4 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 345.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 23.0 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 345.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ag2GeO3 (mp-983589) | 0.5911 | 0.000 | 3 |
AlSbO3 (mvc-3810) | 0.6577 | 0.340 | 3 |
Ca6Al7O16 (mp-721592) | 0.6123 | 0.000 | 3 |
MnPO4 (mp-31942) | 0.6511 | 0.062 | 3 |
SiAg2O3 (mp-28195) | 0.6234 | 0.041 | 3 |
Li3Bi(PO4)2 (mp-760650) | 0.6657 | 0.063 | 4 |
Li2Co2Si2O7 (mp-763369) | 0.6842 | 0.068 | 4 |
LiCuPO4 (mp-25885) | 0.6614 | 0.037 | 4 |
LiCoPO4 (mp-761732) | 0.6814 | 0.070 | 4 |
LiCuPO4 (mp-584808) | 0.6384 | 0.037 | 4 |
Li4Nb2Fe3Te3O16 (mp-765556) | 0.7479 | 0.259 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ca_sv Si O |
Final Energy/Atom-6.9306 eV |
Corrected Energy-570.0795 eV
-570.0795 eV = -540.5833 eV (uncorrected energy) - 29.4962 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)