Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.634 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom< 0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa3Zn(BO2)5 |
Band Gap4.222 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 296.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 197.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 296.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 176.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 98.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 98.9 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 98.9 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 296.6 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 296.6 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 1> | 176.0 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 1> | 176.0 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 197.7 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 296.6 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 1> | 176.0 |
Si (mp-149) | <1 0 0> | <0 0 1> | 296.6 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 197.7 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 296.6 |
CsI (mp-614603) | <1 1 0> | <0 1 1> | 176.0 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 197.7 |
SrTiO3 (mp-4651) | <1 0 0> | <0 1 1> | 176.0 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 296.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 98.9 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 296.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi(BO2)3 (mp-557351) | 0.6321 | 0.017 | 3 |
Bi3B5O12 (mp-23549) | 0.5427 | 0.000 | 3 |
Na2B4O7 (mp-17941) | 0.6141 | 0.000 | 3 |
Bi2B8O15 (mp-542931) | 0.5336 | 0.000 | 3 |
TlBO2 (mp-28244) | 0.5250 | 0.000 | 3 |
Li3MnB6O13 (mp-779068) | 0.4463 | 0.105 | 4 |
Na3Mg(BO2)5 (mp-683990) | 0.1985 | 0.000 | 4 |
Na3Zn(BO2)5 (mp-560158) | 0.2959 | 0.000 | 4 |
Na2ZnB6O11 (mp-1020181) | 0.4419 | 0.003 | 4 |
Na3B5SO8 (mp-560266) | 0.4638 | 0.005 | 4 |
Li2SbAsCO7 (mp-771804) | 0.7100 | 0.064 | 5 |
Li3FePCO7 (mp-767755) | 0.7494 | 0.224 | 5 |
Li3FePCO7 (mp-767347) | 0.7436 | 0.058 | 5 |
Sr2LiBeB3O8 (mp-1020647) | 0.6691 | 0.000 | 5 |
Na2LiB5(PO7)2 (mp-1020146) | 0.5580 | 0.000 | 5 |
NaLiSiB3HO8 (mp-558267) | 0.6480 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Zn B O |
Final Energy/Atom-6.8997 eV |
Corrected Energy-1104.9342 eV
-1104.9342 eV = -1048.7510 eV (uncorrected energy) - 56.1832 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)