Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.696 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZn4B6O13 + Na3B7O12 + ZnO |
Band Gap4.940 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 0 0> | <1 0 0> | 173.9 |
C (mp-48) | <1 0 1> | <1 0 0> | 260.8 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 282.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 244.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 260.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 162.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 162.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 244.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 162.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 260.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 260.8 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 260.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 282.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 162.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 244.2 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 260.8 |
BN (mp-984) | <1 0 0> | <1 0 0> | 173.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 244.2 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 282.2 |
Al (mp-134) | <1 0 0> | <1 0 0> | 260.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 282.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 -1> | 94.1 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 260.8 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 282.2 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 282.2 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <0 0 1> | 162.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 244.2 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 260.8 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 244.2 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 162.8 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 -1> | 282.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 244.2 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 260.8 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 244.2 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 260.8 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 260.8 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 260.8 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 162.8 |
LaF3 (mp-905) | <1 1 0> | <1 0 -1> | 94.1 |
LiAlO2 (mp-3427) | <1 1 0> | <1 0 -1> | 94.1 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 244.2 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 244.2 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 1> | 182.3 |
Si (mp-149) | <1 0 0> | <0 0 1> | 244.2 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 162.8 |
WS2 (mp-224) | <0 0 1> | <1 0 -1> | 282.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 162.8 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 260.8 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 260.8 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 -1> | 282.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.00000 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.72 | 0.00 | 0.07 |
0.00 | 2.54 | -0.00 |
0.07 | -0.00 | 2.43 |
Dielectric Tensor εij (total) |
||
---|---|---|
5.70 | 0.00 | -0.05 |
0.00 | 6.16 | -0.00 |
-0.05 | -0.00 | 7.93 |
Polycrystalline dielectric constant
εpoly∞
2.56
|
Polycrystalline dielectric constant
εpoly
6.60
|
Refractive Index n1.60 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi2B8O15 (mp-542931) | 0.6058 | 0.000 | 3 |
Na12B26O45 (mp-640740) | 0.6262 | 0.009 | 3 |
AgBO2 (mp-559803) | 0.6533 | 0.010 | 3 |
TlBO2 (mp-28244) | 0.6778 | 0.000 | 3 |
Na12B26O45 (mp-657344) | 0.6217 | 0.009 | 3 |
Na3Mg(BO2)5 (mp-683990) | 0.4541 | 0.000 | 4 |
Na3Zn(BO2)5 (mp-560158) | 0.5809 | 0.000 | 4 |
Na3Zn(BO2)5 (mp-1020160) | 0.4419 | 0.000 | 4 |
Cs2Na2B10O17 (mp-559557) | 0.6036 | 0.000 | 4 |
Na3B5SO8 (mp-560266) | 0.6030 | 0.005 | 4 |
Sr2LiBeB3O8 (mp-1020647) | 0.6326 | 0.000 | 5 |
Na2LiB5(PO7)2 (mp-1020146) | 0.5034 | 0.000 | 5 |
NaLiSiB3HO8 (mp-558267) | 0.6839 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Zn B O |
Final Energy/Atom-7.2295 eV |
Corrected Energy-304.6306 eV
-304.6306 eV = -289.1802 eV (uncorrected energy) - 15.4504 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)