Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.057 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap5.522 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 295.9 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 169.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 175.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 98.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 179.5 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 295.9 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 197.3 |
BN (mp-984) | <0 0 1> | <1 0 1> | 175.0 |
Al (mp-134) | <1 0 0> | <1 1 0> | 179.5 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 295.9 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 -1> | 123.0 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 229.3 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 229.3 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 175.0 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 114.6 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 295.9 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 169.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 295.9 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 229.3 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 229.3 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 197.3 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 295.9 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 -1> | 123.0 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 1> | 175.0 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 114.6 |
ZnO (mp-2133) | <1 1 0> | <0 0 1> | 295.9 |
Fe2O3 (mp-24972) | <1 1 0> | <1 0 -1> | 123.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y(PO3)3 (mp-686038) | 0.6328 | 0.481 | 3 |
Sn(PO3)3 (mp-684482) | 0.6447 | 0.125 | 3 |
Sb(PO3)4 (mp-26542) | 0.4913 | 0.037 | 3 |
RbPO3 (mp-4135) | 0.6741 | 0.002 | 3 |
BiP2O7 (mp-672945) | 0.6530 | 0.091 | 3 |
UP3HO11 (mp-703348) | 0.6767 | 0.000 | 4 |
CsUP3O11 (mp-572741) | 0.6241 | 0.000 | 4 |
KUP3O11 (mp-557505) | 0.6954 | 0.000 | 4 |
Cs2B2S3O13 (mp-1019604) | 0.7024 | 0.000 | 4 |
KZnP2O7 (mp-773901) | 0.6797 | 0.087 | 4 |
CsUGa(PO5)2 (mp-559852) | 0.6962 | 0.000 | 5 |
CaP3H10NO12 (mp-705854) | 0.7231 | 0.054 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv B S O |
Final Energy/Atom-6.1236 eV |
Corrected Energy-536.4114 eV
Uncorrected energy = -489.8914 eV
Composition-based energy adjustment (-0.503 eV/atom x 16.0 atoms) = -8.0480 eV
Composition-based energy adjustment (-0.687 eV/atom x 56.0 atoms) = -38.4720 eV
Corrected energy = -536.4114 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)