Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.493 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.703 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZrC + Mg149Zr + C |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinAmm2 [38] |
HallA 2 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 176.3 |
C (mp-48) | <1 0 0> | <0 0 1> | 327.4 |
C (mp-48) | <1 0 1> | <1 0 0> | 202.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 125.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 72.2 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 1> | 125.6 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 125.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 67.6 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 216.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 287.7 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 135.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 176.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 151.1 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 125.6 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 314.0 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 188.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 177.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 226.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 314.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 135.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 144.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 266.4 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 125.6 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 302.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 125.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 176.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 216.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 327.4 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 188.4 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 188.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 177.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 188.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 327.4 |
InP (mp-20351) | <1 1 1> | <1 1 0> | 177.6 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 88.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 327.4 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 226.7 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 277.0 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 302.2 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 201.5 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 201.5 |
CdWO4 (mp-19387) | <1 1 1> | <1 0 0> | 270.6 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 125.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 302.2 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 230.1 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 172.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 327.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 251.8 |
Ni (mp-23) | <1 1 0> | <1 1 1> | 276.9 |
Ni (mp-23) | <1 1 1> | <1 1 1> | 276.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaMg6Fe (mp-1099278) | 0.4078 | 0.391 | 3 |
CeMg6C (mp-1021162) | 0.2853 | 0.476 | 3 |
CeMg6B (mp-1098076) | 0.2844 | 0.382 | 3 |
Re2Si (mp-669547) | 0.5783 | 0.313 | 2 |
MgSi2 (mp-1073469) | 0.5702 | 0.252 | 2 |
Mg4Si3 (mp-1074279) | 0.5570 | 0.178 | 2 |
Mg4Si3 (mp-1074349) | 0.5274 | 0.204 | 2 |
Mg4Si3 (mp-1074526) | 0.5799 | 0.167 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Zr_sv C |
Final Energy/Atom-2.9286 eV |
Corrected Energy-23.4290 eV
-23.4290 eV = -23.4290 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)