Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.040 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.094 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYMg149 + YMg3 + Hf |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmmm [65] |
Hall-C 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 77.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 237.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 86.0 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 192.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 305.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 190.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 258.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 86.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 271.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 230.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 230.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 192.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 190.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 192.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 190.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 154.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 285.1 |
C (mp-48) | <0 0 1> | <0 1 0> | 346.6 |
C (mp-48) | <1 0 0> | <0 1 0> | 38.5 |
C (mp-48) | <1 0 1> | <1 0 0> | 237.6 |
C (mp-48) | <1 1 0> | <0 1 1> | 172.1 |
C (mp-48) | <1 1 1> | <0 1 0> | 231.1 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 1> | 294.8 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 230.8 |
Te2Mo (mp-602) | <1 1 0> | <0 1 0> | 192.6 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 192.6 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 332.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 237.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 332.6 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 77.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 230.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 190.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 172.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 190.0 |
BN (mp-984) | <1 1 0> | <0 1 1> | 172.1 |
BN (mp-984) | <1 1 1> | <0 1 1> | 172.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 269.6 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 172.1 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 192.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 230.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 285.1 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 237.6 |
Al (mp-134) | <1 0 0> | <0 1 0> | 192.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 230.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 230.8 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 192.6 |
CdWO4 (mp-19387) | <0 1 1> | <1 1 1> | 196.5 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 180.8 |
Al (mp-134) | <1 1 1> | <1 0 0> | 190.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 346.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2CuGe (mp-676117) | 0.3663 | 0.008 | 3 |
FeSnRh2 (mp-1018062) | 0.7483 | 0.000 | 3 |
MnGaNi2 (mp-604537) | 0.7128 | 0.007 | 3 |
Al2CuIr (mp-1079890) | 0.6918 | 0.000 | 3 |
Hf2Zn (mp-1014231) | 0.2620 | 0.000 | 2 |
Ru3Cl (mp-974467) | 0.2621 | 1.142 | 2 |
MnPd (mp-238) | 0.2629 | 0.002 | 2 |
TaRu (mp-1601) | 0.2718 | 0.000 | 2 |
NbRu (mp-432) | 0.2657 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Hf_pv Mg_pv |
Final Energy/Atom-3.2133 eV |
Corrected Energy-25.7064 eV
-25.7064 eV = -25.7064 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)