Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.386 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.079 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + Te2W + MoWSe4 |
Band Gap1.039 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 71.5 |
C (mp-48) | <1 0 0> | <0 0 1> | 255.3 |
C (mp-48) | <1 0 1> | <0 0 1> | 337.0 |
C (mp-48) | <1 1 0> | <0 0 1> | 245.1 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 316.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 132.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 251.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 275.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 173.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 326.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 163.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 163.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 357.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 275.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 71.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 91.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 194.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 253.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 286.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 71.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 286.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 337.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 194.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 163.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 183.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 204.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 194.0 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 245.1 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 245.1 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 194.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 245.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 163.4 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 167.6 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 251.5 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 316.6 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 255.3 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 132.8 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 224.7 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 234.9 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 316.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 214.5 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 71.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 132.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 286.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 275.7 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 286.0 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 61.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 122.6 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 194.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Te2Mo3Se4 (mp-1025876) | 0.0664 | 0.025 | 3 |
W3(SeS2)2 (mp-1025577) | 0.0697 | 0.013 | 3 |
TeMoSe (mp-1023948) | 0.0198 | 0.029 | 3 |
TeWSe (mp-1023943) | 0.0104 | 0.044 | 3 |
TeMoSe (mp-1030732) | 0.0678 | 0.028 | 3 |
Te4Mo3WSe4 (mp-1030615) | 0.0679 | 0.091 | 4 |
Te2Mo2WSe4 (mp-1025885) | 0.0676 | 0.136 | 4 |
Te2Mo2WSe4 (mp-1025779) | 0.0659 | 0.109 | 4 |
Te2MoWSe2 (mp-1023945) | 0.0237 | 0.118 | 4 |
Te4Mo3WSe4 (mp-1030736) | 0.0684 | 0.110 | 4 |
WS2 (mp-1028441) | 0.1863 | 0.001 | 2 |
WSe2 (mp-1025572) | 0.1850 | 0.000 | 2 |
WS2 (mp-1025571) | 0.1849 | 0.001 | 2 |
MoSe2 (mp-1023940) | 0.1831 | 0.000 | 2 |
WSe2 (mp-1023933) | 0.1806 | 0.001 | 2 |
Te4MoW3(SeS)2 (mp-1030574) | 0.1389 | 0.110 | 5 |
Te2MoWSeS (mp-1030534) | 0.1370 | 0.103 | 5 |
Te2MoWSeS (mp-1030176) | 0.1335 | 0.083 | 5 |
Te2MoWSeS (mp-1028919) | 0.1380 | 0.118 | 5 |
Te4Mo3W(SeS)2 (mp-1027133) | 0.1357 | 0.116 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv Se |
Final Energy/Atom-6.5665 eV |
Corrected Energy-39.3992 eV
-39.3992 eV = -39.3992 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)