Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.714 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.078 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + MoS2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 273.8 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 312.9 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 312.9 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 303.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 127.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 273.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 273.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 322.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 205.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 68.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 117.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 48.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 117.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 29.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 264.0 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 312.9 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 312.9 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 97.8 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 127.1 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 332.5 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 185.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 68.4 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 303.1 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 127.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 381.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 127.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 156.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 107.6 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 264.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 224.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 264.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 185.8 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 215.1 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 273.8 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 361.8 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 273.8 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 68.4 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 185.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 273.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 303.1 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 97.8 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 136.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 68.4 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 303.1 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 97.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 136.9 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 264.0 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 234.7 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 342.2 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 273.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeMoS (mp-1027412) | 0.0614 | 0.078 | 3 |
TeWS (mp-1028690) | 0.0686 | 0.097 | 3 |
TeWS (mp-1028526) | 0.0646 | 0.097 | 3 |
TeMoS (mp-1027738) | 0.0583 | 0.078 | 3 |
TeWS (mp-1023931) | 0.0216 | 0.096 | 3 |
Te4Mo3WS4 (mp-1027132) | 0.0633 | 0.115 | 4 |
Te4Mo3WS4 (mp-1027911) | 0.0615 | 0.117 | 4 |
Te2MoWS2 (mp-1027615) | 0.0622 | 0.155 | 4 |
Te2MoWS2 (mp-1023963) | 0.0123 | 0.155 | 4 |
Te2MoWS2 (mp-1023932) | 0.0186 | 0.082 | 4 |
MoS2 (mp-1025874) | 0.3314 | 0.001 | 2 |
WS2 (mp-1025571) | 0.3374 | 0.001 | 2 |
MoS2 (mp-1023939) | 0.3323 | 0.001 | 2 |
WS2 (mp-1023925) | 0.3370 | 0.001 | 2 |
MoS2 (mp-1027525) | 0.3313 | 0.001 | 2 |
Te2Mo2W(SeS)2 (mp-1026027) | 0.0684 | 0.135 | 5 |
Te2Mo2W(SeS)2 (mp-1026016) | 0.0691 | 0.105 | 5 |
Te2Mo2W(SeS)2 (mp-1025933) | 0.0674 | 0.107 | 5 |
Te2MoW2(SeS)2 (mp-1025836) | 0.0688 | 0.137 | 5 |
Te2MoW2(SeS)2 (mp-1025722) | 0.0723 | 0.116 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv S |
Final Energy/Atom-6.5346 eV |
Corrected Energy-40.5343 eV
-40.5343 eV = -39.2074 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)