Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.601 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.071 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaAlO3 + Al2O3 |
Band Gap4.351 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 0 0> | <0 0 1> | 197.0 |
C (mp-48) | <1 0 1> | <0 0 1> | 328.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 262.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 328.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 129.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 197.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 328.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 328.3 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 197.0 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 -1> | 122.7 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 -1> | 122.7 |
Ni (mp-23) | <1 0 0> | <1 0 -1> | 122.7 |
Ni (mp-23) | <1 1 1> | <1 0 1> | 129.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 65.7 |
BN (mp-984) | <1 0 1> | <1 0 1> | 258.0 |
Al (mp-134) | <1 1 0> | <0 0 1> | 328.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 197.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 65.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 328.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 262.7 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 197.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 262.7 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 214.8 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 197.0 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 328.3 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 328.3 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 197.0 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 328.3 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 214.8 |
MgF2 (mp-1249) | <1 0 0> | <1 0 -1> | 245.4 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 262.7 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 214.8 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 0> | 214.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 107.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 245.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 214.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 328.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 258.0 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 122.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 262.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 197.0 |
Al (mp-134) | <1 1 1> | <1 0 1> | 258.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 129.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 197.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 328.3 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 214.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 258.0 |
YVO4 (mp-19133) | <1 1 1> | <1 0 -1> | 245.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 262.7 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 0> | 214.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tm4(B2O5)3 (mp-772919) | 0.5630 | 0.021 | 3 |
Er4(B2O5)3 (mp-772497) | 0.5678 | 0.041 | 3 |
Bi4(B2O5)3 (mp-768923) | 0.5353 | 0.005 | 3 |
Lu4(B2O5)3 (mp-771772) | 0.5371 | 0.039 | 3 |
La4Al6O15 (mp-771838) | 0.1275 | 0.074 | 3 |
K2LiNbO4 (mp-759900) | 0.7178 | 0.000 | 4 |
Rb2Ga2Ge3O10 (mp-752475) | 0.6714 | 0.084 | 4 |
LiBiB2O5 (mp-755835) | 0.6291 | 0.102 | 4 |
K4Li3Mn2O8 (mp-762647) | 0.7277 | 0.066 | 4 |
NaVTeO5 (mp-18897) | 0.7097 | 0.000 | 4 |
Sr3Li3Cu3(PO4)4 (mp-780775) | 0.7370 | 0.099 | 5 |
CeBeSiHO5 (mp-686671) | 0.7440 | 0.220 | 5 |
KNa3Al4(GeO4)4 (mp-573281) | 0.7384 | 0.336 | 5 |
NaCaBeSi2O6F (mp-560721) | 0.7244 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Al O |
Final Energy/Atom-7.8372 eV |
Corrected Energy-412.9263 eV
-412.9263 eV = -391.8576 eV (uncorrected energy) - 21.0687 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)