Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.730 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.807 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mcm [140] |
Hall-I 4 2c |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 190.7 |
C (mp-48) | <1 0 0> | <1 0 0> | 94.3 |
C (mp-48) | <1 0 1> | <0 0 1> | 305.1 |
C (mp-48) | <1 1 0> | <1 1 0> | 66.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 305.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 242.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 235.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 190.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 141.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 330.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 152.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 330.2 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 200.1 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 94.3 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 190.7 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 94.3 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 1> | 182.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 343.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 305.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 38.1 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 266.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 267.0 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 266.8 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 235.9 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 200.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 200.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 330.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 267.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 343.3 |
BN (mp-984) | <0 0 1> | <1 1 0> | 266.8 |
BN (mp-984) | <1 1 0> | <1 1 0> | 66.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 267.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 152.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 330.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 38.1 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 266.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 305.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 200.1 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 343.3 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 305.1 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 305.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 152.6 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 266.8 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 94.3 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 330.2 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 235.9 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 190.7 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 76.3 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 182.0 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 182.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
13.72 | -0.00 | 0.00 |
-0.00 | 13.72 | 0.00 |
0.00 | 0.00 | 13.08 |
Dielectric Tensor εij (total) |
||
---|---|---|
58.29 | -0.00 | 0.00 |
-0.00 | 58.29 | -0.00 |
0.00 | -0.00 | 137.38 |
Polycrystalline dielectric constant
εpoly∞
13.51
|
Polycrystalline dielectric constant
εpoly
84.65
|
Refractive Index n3.68 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiNO3 (mp-696822) | 0.7278 | 1.117 | 3 |
YbOF (mp-7028) | 0.7316 | 0.000 | 3 |
KPrTe4 (mp-11132) | 0.7266 | 0.007 | 3 |
FeSeN (mp-1071360) | 0.7241 | 1.378 | 3 |
KCeSe4 (mp-22395) | 0.7007 | 0.012 | 3 |
PbSe2 (mp-982261) | 0.2384 | 0.054 | 2 |
BaTe2 (mp-2150) | 0.3609 | 0.002 | 2 |
SrS2 (mp-1950) | 0.0948 | 0.011 | 2 |
IrC2 (mp-1077157) | 0.3763 | 1.415 | 2 |
TiN2 (mp-1080172) | 0.1162 | 0.268 | 2 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pb_d S |
Final Energy/Atom-4.2824 eV |
Corrected Energy-28.3483 eV
-28.3483 eV = -25.6945 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)