Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.197 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.055 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToUMoC2 + Mo + U |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 0 -1> | 140.5 |
C (mp-48) | <1 0 1> | <1 0 -1> | 175.6 |
C (mp-48) | <1 1 1> | <1 0 0> | 264.4 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 52.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 299.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 229.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 88.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 280.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 175.6 |
C (mp-48) | <1 0 0> | <1 0 -1> | 175.6 |
C (mp-48) | <1 1 0> | <1 0 0> | 264.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 158.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 17.6 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 47.1 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 35.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 141.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 123.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 370.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 141.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 193.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 263.5 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 175.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 264.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 158.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 88.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 282.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 229.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 245.8 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 280.9 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 280.9 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 280.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 88.1 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 334.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 229.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 150.6 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 301.1 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 235.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 158.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 144.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 88.1 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 185.0 |
CdWO4 (mp-19387) | <0 1 1> | <1 0 -1> | 245.8 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 225.8 |
CdWO4 (mp-19387) | <1 1 0> | <1 0 -1> | 280.9 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 370.2 |
InP (mp-20351) | <1 1 1> | <1 0 -1> | 245.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 140.5 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 334.9 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 94.3 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 301.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pu2W2C3 (mp-1025268) | 0.2910 | 0.030 | 3 |
U2Re2C3 (mp-1025230) | 0.1032 | 0.000 | 3 |
Ce2Mo2C3 (mp-13263) | 0.4583 | 0.000 | 3 |
U2Re2C3 (mp-1078133) | 0.4479 | 0.100 | 3 |
U2Mo2C3 (mp-1078036) | 0.4535 | 0.124 | 3 |
Li3Ti2Cu3O10 (mp-849652) | 0.7171 | 0.090 | 4 |
Li5WNO4 (mp-772397) | 0.7377 | 0.049 | 4 |
Li2V(OF)2 (mp-764218) | 0.7185 | 0.089 | 4 |
Li4Co(OF)2 (mp-853163) | 0.6935 | 0.084 | 4 |
Li3Ti2Mn3O10 (mp-762872) | 0.7145 | 0.047 | 4 |
Sr4N3 (mp-685023) | 0.6653 | 0.232 | 2 |
Cr3N4 (mp-1014365) | 0.7372 | 0.200 | 2 |
Fe3O4 (mp-705416) | 0.7273 | 0.128 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U Mo_pv C |
Final Energy/Atom-10.4832 eV |
Corrected Energy-73.3823 eV
-73.3823 eV = -73.3823 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)