Final Magnetic Moment-0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.279 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.031 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density16.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPt + SiPt2 + Ag |
Band Gap0.046 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mmm [123] |
Hall-P 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 173.4 |
C (mp-48) | <1 1 1> | <0 0 1> | 315.3 |
C (mp-48) | <1 0 0> | <0 0 1> | 220.7 |
C (mp-48) | <1 0 1> | <0 0 1> | 252.2 |
C (mp-48) | <1 1 0> | <1 1 1> | 129.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 283.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 254.6 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 160.1 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 344.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 236.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 31.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 129.6 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 129.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 157.6 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 226.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 31.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 226.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 78.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 252.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 200.1 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 200.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 86.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 78.8 |
KCl (mp-23193) | <1 1 0> | <1 1 1> | 172.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 31.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 280.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 220.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 129.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 160.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 63.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 78.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 31.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 226.4 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 226.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 15.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 110.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 141.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 141.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 236.5 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 120.0 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 113.2 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 1> | 129.0 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 315.3 |
CdWO4 (mp-19387) | <1 1 1> | <1 1 0> | 160.1 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 236.5 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 1> | 129.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 204.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 204.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 283.7 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 63.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AgPPt5 (mp-1025385) | 0.0485 | 0.012 | 3 |
InSiPt5 (mp-1025370) | 0.0469 | 0.000 | 3 |
MgPPd5 (mp-1025261) | 0.1024 | 0.000 | 3 |
CdPPt5 (mp-1025187) | 0.0898 | 0.000 | 3 |
SiSbPt5 (mp-1025366) | 0.1027 | 0.017 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points12 |
U Values-- |
PseudopotentialsVASP PAW: Si Ag Pt |
Final Energy/Atom-5.7839 eV |
Corrected Energy-40.4873 eV
-40.4873 eV = -40.4873 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)