Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.452 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHo3Ge5 + Ge |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 0 0> | <0 1 0> | 95.3 |
C (mp-48) | <1 1 0> | <1 0 0> | 164.9 |
C (mp-48) | <1 1 1> | <0 1 0> | 238.1 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 301.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 301.6 |
C (mp-48) | <0 0 1> | <0 1 0> | 206.4 |
C (mp-48) | <1 0 1> | <0 1 0> | 222.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 251.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 285.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 63.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 168.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 235.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 168.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 111.1 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 247.3 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 0> | 317.5 |
CdWO4 (mp-19387) | <1 1 1> | <0 1 0> | 206.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 174.6 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 63.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 301.6 |
BN (mp-984) | <0 0 1> | <0 1 0> | 158.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 285.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 349.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 158.8 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 349.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 238.1 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 222.3 |
MoS2 (mp-1434) | <1 1 0> | <1 0 1> | 117.9 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 269.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 127.0 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 158.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 168.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 235.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 168.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 269.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 317.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 222.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 301.6 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 251.9 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 381.0 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 254.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 238.0 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 333.4 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 235.8 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 142.9 |
TeO2 (mp-2125) | <1 1 0> | <0 1 0> | 95.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 127.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 158.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 222.3 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 333.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CeAgP2 (mp-675111) | 0.7383 | 0.222 | 3 |
K3SnSb3 (mp-675476) | 0.6920 | 0.092 | 3 |
Ni5Ge2P3 (mp-662818) | 0.6903 | 0.043 | 3 |
Si2Ni5P3 (mp-649521) | 0.6737 | 0.051 | 3 |
Tl3PbCl5 (mp-30519) | 0.7434 | 0.009 | 3 |
ErGe3 (mp-513) | 0.0531 | 0.006 | 2 |
TbGe3 (mp-1025491) | 0.0595 | 0.019 | 2 |
YGe3 (mp-29772) | 0.0325 | 0.019 | 2 |
TmGe3 (mp-1078795) | 0.0652 | 0.019 | 2 |
DyGe3 (mp-21159) | 0.0249 | 0.018 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ho_3 Ge_d |
Final Energy/Atom-5.0607 eV |
Corrected Energy-40.4856 eV
-40.4856 eV = -40.4856 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)