Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.808 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 256.7 |
C (mp-48) | <1 0 0> | <1 1 1> | 157.1 |
C (mp-48) | <1 0 1> | <0 0 1> | 171.2 |
C (mp-48) | <1 1 0> | <0 1 0> | 168.1 |
C (mp-48) | <1 1 1> | <1 0 1> | 176.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 149.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 213.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 149.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 149.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 196.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 107.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 107.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 116.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 88.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 42.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 256.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 132.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 192.5 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 286.8 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 317.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 171.2 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 209.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 154.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 107.0 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 334.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 192.5 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 105.8 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 246.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 171.2 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 209.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 64.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 42.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 107.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 192.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 132.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 278.1 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 191.2 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 282.0 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 209.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 132.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 192.5 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 286.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 64.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 112.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 278.1 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 221.2 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 308.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 271.0 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 282.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 116.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2NiP (mp-5918) | 0.4616 | 0.000 | 3 |
Zr2CoP (mp-29152) | 0.5306 | 0.000 | 3 |
Zr2NiP (mp-29153) | 0.5460 | 0.000 | 3 |
Hf2CoP (mp-29154) | 0.4476 | 0.000 | 3 |
Zr2Nb3Ge4 (mp-540755) | 0.6303 | 0.082 | 3 |
SrCa2In2Ge (mp-619206) | 0.4788 | 0.106 | 4 |
TiSi (mp-7092) | 0.1297 | 0.000 | 2 |
HfSi (mp-1042) | 0.1858 | 0.000 | 2 |
ZrSi (mp-893) | 0.2435 | 0.000 | 2 |
ScGa (mp-11411) | 0.3237 | 0.000 | 2 |
ZrGa (mp-30682) | 0.3256 | 0.000 | 2 |
Si (mp-1001113) | 0.6094 | 0.488 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zr_sv Ge_d |
Final Energy/Atom-7.3905 eV |
Corrected Energy-59.1237 eV
-59.1237 eV = -59.1237 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)