Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.571 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 0 1> | <0 1 0> | 302.2 |
C (mp-48) | <0 0 1> | <0 1 0> | 302.2 |
C (mp-48) | <1 0 0> | <0 1 1> | 133.1 |
C (mp-48) | <1 1 0> | <0 1 0> | 264.5 |
C (mp-48) | <1 1 1> | <0 1 0> | 264.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 75.6 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 75.6 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 264.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 96.6 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 199.7 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 266.2 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 113.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 340.0 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 199.7 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 302.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 219.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 274.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 226.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 188.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 188.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 96.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 96.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 188.9 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 264.5 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 113.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 274.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 264.5 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 266.2 |
CdWO4 (mp-19387) | <1 0 0> | <0 1 0> | 226.7 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 302.2 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 219.2 |
CdWO4 (mp-19387) | <1 1 1> | <0 1 1> | 199.7 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 133.1 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 302.2 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 75.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 75.6 |
Ni (mp-23) | <1 0 0> | <0 1 1> | 199.7 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 193.3 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 332.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 226.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 274.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 274.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 328.8 |
Al (mp-134) | <1 0 0> | <1 0 0> | 96.6 |
Al (mp-134) | <1 1 0> | <0 1 0> | 188.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 264.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 226.7 |
CdTe (mp-406) | <1 0 0> | <0 1 1> | 133.1 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 302.2 |
CdTe (mp-406) | <1 1 1> | <0 1 0> | 75.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YAl2Co (mp-16493) | 0.1609 | 0.000 | 3 |
YbAl2Ni (mp-12782) | 0.2751 | 0.000 | 3 |
BaIn2Rh (mp-11078) | 0.1760 | 0.000 | 3 |
BaIn2Pt (mp-21032) | 0.1298 | 0.000 | 3 |
BaIn2Ir (mp-22780) | 0.2179 | 0.000 | 3 |
MgH2 (mp-23712) | 0.6137 | 0.082 | 2 |
PRu2 (mp-21911) | 0.6654 | 0.000 | 2 |
KGe (mp-2146) | 0.6553 | 0.041 | 2 |
CsSn (mp-571056) | 0.6369 | 0.000 | 2 |
Mg3Si4 (mp-1075020) | 0.5912 | 0.229 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv In_d Pd |
Final Energy/Atom-3.7205 eV |
Corrected Energy-29.7642 eV
Uncorrected energy = -29.7642 eV
Corrected energy = -29.7642 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)