Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.971 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.088 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 1 1> | 291.0 |
C (mp-48) | <1 1 0> | <0 0 1> | 166.8 |
C (mp-48) | <1 0 0> | <1 1 -1> | 170.2 |
C (mp-48) | <1 0 1> | <1 0 -1> | 261.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 144.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 247.9 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 250.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 139.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 240.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 139.0 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 234.6 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 240.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 83.4 |
CeO2 (mp-20194) | <1 1 1> | <1 1 -1> | 255.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 240.3 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 267.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 117.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 55.6 |
BaF2 (mp-1029) | <1 1 1> | <1 0 -1> | 208.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 111.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 305.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 111.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 333.7 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 117.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 55.6 |
KCl (mp-23193) | <1 1 1> | <1 0 -1> | 208.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 250.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 336.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 336.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 -1> | 208.8 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 117.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 55.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 333.7 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 267.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 361.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 250.3 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 305.9 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 176.0 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 218.2 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 240.3 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 194.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 111.2 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 194.7 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 333.7 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 -1> | 261.0 |
CdWO4 (mp-19387) | <1 1 0> | <1 0 0> | 336.4 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 278.1 |
CdWO4 (mp-19387) | <0 1 1> | <1 0 0> | 336.4 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 278.1 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 176.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb(ThSe3)2 (mp-9523) | 0.6020 | 0.000 | 3 |
HfSiTe (mp-13963) | 0.6603 | 0.000 | 3 |
K(USe3)2 (mp-12414) | 0.6103 | 0.000 | 3 |
ZrSiTe (mp-19917) | 0.6580 | 0.000 | 3 |
U2TlSe6 (mp-1078777) | 0.6497 | 0.000 | 3 |
CeMnSbO (mp-542723) | 0.6604 | 0.108 | 4 |
LaMnSbO (mp-18745) | 0.6858 | 0.043 | 4 |
SmMnSbO (mp-510488) | 0.6275 | 0.090 | 4 |
NdMnSbO (mp-18755) | 0.6451 | 0.068 | 4 |
CeZnSbO (mp-909296) | 0.6928 | 0.022 | 4 |
USe3 (mp-909149) | 0.2872 | 0.018 | 2 |
UTe3 (mp-8357) | 0.2765 | 0.042 | 2 |
USe3 (mp-9429) | 0.2519 | 0.018 | 2 |
HfSe3 (mp-15622) | 0.2670 | 0.000 | 2 |
ZrSe3 (mp-1683) | 0.2094 | 0.000 | 2 |
SrNd7Fe8(AsO)8 (mp-705458) | 0.7482 | 0.208 | 5 |
Sm6Fe6As6O5F (mp-697821) | 0.7434 | 0.170 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Th Te |
Final Energy/Atom-5.1816 eV |
Corrected Energy-41.4530 eV
-41.4530 eV = -41.4530 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)