Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.343 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.059 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + Te2W + MoWSe4 |
Band Gap0.886 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6m2 [187] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 136.0 |
C (mp-48) | <1 0 0> | <0 0 1> | 334.7 |
C (mp-48) | <1 0 1> | <0 0 1> | 292.9 |
C (mp-48) | <1 1 0> | <0 0 1> | 324.3 |
C (mp-48) | <1 1 1> | <0 0 1> | 303.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 73.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 73.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 261.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 125.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 282.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 177.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 240.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 282.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 198.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 167.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 282.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 198.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 198.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 282.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 292.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 73.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 292.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 261.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 188.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 198.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 167.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 198.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 209.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 198.7 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 104.6 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 251.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 111.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 272.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 292.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 209.2 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 324.3 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 292.9 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 313.8 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 240.6 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 324.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 219.7 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 73.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 10.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 272.0 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 111.4 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 272.0 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 94.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 62.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 188.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 198.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Te3Mo2Se (mp-1030447) | 0.0531 | 0.021 | 3 |
WSeS (mp-1028663) | 0.0532 | 0.014 | 3 |
Te3W2Se (mp-1028598) | 0.0507 | 0.042 | 3 |
Te4W3Se2 (mp-1026356) | 0.0107 | 0.044 | 3 |
Te4Mo3Se2 (mp-1025685) | 0.0133 | 0.025 | 3 |
Te3MoWSe (mp-1030161) | 0.0488 | 0.052 | 4 |
Te6MoW3Se2 (mp-1028583) | 0.0484 | 0.059 | 4 |
Te4Mo(WSe)2 (mp-1025682) | 0.0102 | 0.068 | 4 |
Te4Mo2WSe2 (mp-1025626) | 0.0163 | 0.084 | 4 |
Te4Mo(WSe)2 (mp-1025585) | 0.0143 | 0.093 | 4 |
Te2Mo (mp-1030319) | 0.1838 | 0.000 | 2 |
WSe2 (mp-1028698) | 0.1807 | 0.000 | 2 |
Te2Mo (mp-1025576) | 0.1777 | 0.000 | 2 |
WSe2 (mp-1025572) | 0.1786 | 0.000 | 2 |
Te2Mo (mp-1023938) | 0.1815 | 0.001 | 2 |
Te4Mo3W(SeS)2 (mp-1030450) | 0.1505 | 0.082 | 5 |
Te4Mo3W(SeS)2 (mp-1030284) | 0.1560 | 0.098 | 5 |
Te4MoW3(SeS)2 (mp-1029233) | 0.1596 | 0.092 | 5 |
Te2MoWSeS (mp-1029213) | 0.1512 | 0.083 | 5 |
Te4MoW3(SeS)2 (mp-1028626) | 0.1596 | 0.111 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv Se |
Final Energy/Atom-6.3665 eV |
Corrected Energy-57.2984 eV
-57.2984 eV = -57.2984 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)