Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.818 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.096 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToWS2 + MoWSe4 |
Band Gap0.723 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 37.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 297.2 |
C (mp-48) | <1 0 1> | <0 0 1> | 157.9 |
C (mp-48) | <1 1 0> | <0 0 1> | 222.9 |
C (mp-48) | <1 1 1> | <0 0 1> | 343.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 176.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 232.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 111.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 250.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 260.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 371.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 148.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 167.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 315.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 176.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 195.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 204.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 139.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 325.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 297.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 297.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 287.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 92.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 362.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 222.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 195.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 260.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 167.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 315.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 176.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 176.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 111.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 325.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 250.7 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 65.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 213.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 260.0 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 213.6 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 232.1 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 120.7 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 297.2 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 260.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 297.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 185.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
W2Se3S (mp-1028686) | 0.0407 | 0.011 | 3 |
WSeS (mp-1028663) | 0.0369 | 0.014 | 3 |
MoSeS (mp-1026916) | 0.0279 | 0.014 | 3 |
Mo3(Se2S)2 (mp-1025819) | 0.0233 | 0.012 | 3 |
W3(Se2S)2 (mp-1025588) | 0.0081 | 0.013 | 3 |
Mo3W(SeS)4 (mp-1026927) | 0.0309 | 0.059 | 4 |
Mo3W(SeS)4 (mp-1026909) | 0.0326 | 0.076 | 4 |
Mo2W(Se2S)2 (mp-1025841) | 0.0186 | 0.095 | 4 |
Mo2W(Se2S)2 (mp-1025748) | 0.0104 | 0.073 | 4 |
MoW2(Se2S)2 (mp-1025589) | 0.0119 | 0.118 | 4 |
WS2 (mp-1028441) | 0.1515 | 0.001 | 2 |
Te2Mo (mp-1025576) | 0.1519 | 0.000 | 2 |
WSe2 (mp-1025572) | 0.1521 | 0.000 | 2 |
WS2 (mp-1025571) | 0.1518 | 0.001 | 2 |
Te2Mo (mp-1023938) | 0.1516 | 0.001 | 2 |
Te4Mo3W(SeS)2 (mp-1030450) | 0.1866 | 0.082 | 5 |
Te4Mo3W(SeS)2 (mp-1030404) | 0.1954 | 0.116 | 5 |
Te4Mo3W(SeS)2 (mp-1030284) | 0.1897 | 0.098 | 5 |
Te2MoWSeS (mp-1029213) | 0.1878 | 0.083 | 5 |
Te4MoW3(SeS)2 (mp-1028626) | 0.1957 | 0.111 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mo_pv W_pv Se S |
Final Energy/Atom-7.2279 eV |
Corrected Energy-66.3782 eV
-66.3782 eV = -65.0512 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)