Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.856 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.073 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoWSe4 + MoS2 |
Band Gap0.915 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 37.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 297.1 |
C (mp-48) | <1 0 1> | <0 0 1> | 157.8 |
C (mp-48) | <1 1 0> | <0 0 1> | 222.8 |
C (mp-48) | <1 1 1> | <0 0 1> | 343.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 176.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 232.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 111.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 250.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 260.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 371.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 148.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 167.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 315.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 176.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 195.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 204.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 139.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 325.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 297.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 297.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 287.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 92.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 362.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 222.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 195.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 260.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 167.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 315.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 176.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 176.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 111.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 325.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 250.7 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 65.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 213.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 260.0 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 213.5 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 232.1 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 120.7 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 222.8 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 297.1 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 260.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 297.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
W2Se3S (mp-1028769) | 0.0406 | 0.011 | 3 |
WSeS (mp-1028764) | 0.0470 | 0.015 | 3 |
Mo3(Se2S)2 (mp-1025906) | 0.0197 | 0.013 | 3 |
W3(Se2S)2 (mp-1025599) | 0.0119 | 0.013 | 3 |
MoSeS (mp-1027580) | 0.0355 | 0.014 | 3 |
Mo2W(Se2S)2 (mp-1025946) | 0.0197 | 0.096 | 4 |
Mo2W(Se2S)2 (mp-1025866) | 0.0180 | 0.096 | 4 |
MoW2(Se2S)2 (mp-1025870) | 0.0146 | 0.118 | 4 |
MoW2(Se2S)2 (mp-1025816) | 0.0110 | 0.096 | 4 |
MoW2(Se2S)2 (mp-1025656) | 0.0101 | 0.096 | 4 |
WS2 (mp-1028441) | 0.1514 | 0.001 | 2 |
WS2 (mp-1025571) | 0.1530 | 0.001 | 2 |
WS2 (mp-1023925) | 0.1619 | 0.001 | 2 |
MoS2 (mp-1027525) | 0.1775 | 0.001 | 2 |
NbSe2 (mp-568347) | 0.1688 | 0.007 | 2 |
Te4Mo3W(SeS)2 (mp-1030576) | 0.1849 | 0.082 | 5 |
Te4Mo3W(SeS)2 (mp-1030338) | 0.1812 | 0.097 | 5 |
Te4Mo3W(SeS)2 (mp-1030252) | 0.1866 | 0.097 | 5 |
Te2MoWSeS (mp-1030176) | 0.1827 | 0.083 | 5 |
Te2MoWSeS (mp-1029121) | 0.1890 | 0.084 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mo_pv W_pv Se S |
Final Energy/Atom-7.0314 eV |
Corrected Energy-66.1767 eV
Uncorrected energy = -63.2827 eV
Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV
Composition-based energy adjustment (-0.472 eV/atom x 4.0 atoms) = -1.8880 eV
Corrected energy = -66.1767 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)