Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.634 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.084 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoSe2 + MoWSe4 |
Band Gap1.230 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 182.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 229.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 162.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 229.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 182.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 239.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 201.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 38.3 |
C (mp-48) | <1 0 0> | <0 0 1> | 277.8 |
C (mp-48) | <1 0 1> | <0 0 1> | 162.9 |
C (mp-48) | <1 1 0> | <0 0 1> | 229.9 |
C (mp-48) | <1 1 1> | <0 0 1> | 354.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 95.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 67.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 229.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 229.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 182.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 28.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 239.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 115.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 239.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 239.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 335.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 153.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 229.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 201.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 67.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 268.2 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 268.2 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 220.3 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 335.3 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 239.5 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 268.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 67.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 143.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 67.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 306.5 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 297.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 134.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 268.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 124.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 268.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 268.2 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 201.2 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 143.7 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 67.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 67.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 47.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 115.0 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 182.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MoW3Se8 (mp-1028823) | 0.0315 | 0.063 | 3 |
Mo3WSe8 (mp-1028420) | 0.0318 | 0.063 | 3 |
Mo2WSe6 (mp-1025815) | 0.0128 | 0.084 | 3 |
Mo(WSe3)2 (mp-1025787) | 0.0083 | 0.084 | 3 |
Mo(WSe3)2 (mp-1025575) | 0.0197 | 0.084 | 3 |
MoWSeS3 (mp-1027391) | 0.1329 | 0.034 | 4 |
MoW3(SeS3)2 (mp-1029037) | 0.1242 | 0.034 | 4 |
MoWSeS3 (mp-1027292) | 0.1329 | 0.034 | 4 |
MoW2(SeS2)2 (mp-1025663) | 0.1320 | 0.043 | 4 |
Mo3W(SeS3)2 (mp-1027472) | 0.1334 | 0.033 | 4 |
Te2Mo (mp-1030319) | 0.0520 | 0.000 | 2 |
Te2Mo (mp-1025576) | 0.0390 | 0.000 | 2 |
Te2W (mp-1025573) | 0.0582 | 0.026 | 2 |
Te2W (mp-1023942) | 0.0610 | 0.026 | 2 |
Te2Mo (mp-1023938) | 0.0538 | 0.001 | 2 |
Te4Mo3W(SeS)2 (mp-1030576) | 0.2945 | 0.082 | 5 |
Te2Mo3W(Se2S)2 (mp-1030575) | 0.2958 | 0.087 | 5 |
Te4Mo3W(SeS)2 (mp-1030338) | 0.2903 | 0.097 | 5 |
Te2MoWSeS (mp-1030176) | 0.2857 | 0.083 | 5 |
Te2MoWSeS (mp-1029121) | 0.2934 | 0.084 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mo_pv W_pv Se |
Final Energy/Atom-6.8142 eV |
Corrected Energy-64.1594 eV
Uncorrected energy = -61.3274 eV
Composition-based energy adjustment (-0.472 eV/atom x 6.0 atoms) = -2.8320 eV
Corrected energy = -64.1594 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)