Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.699 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.053 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + MoSe2 + MoS2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 242.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 242.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 165.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 340.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 155.4 |
C (mp-48) | <0 0 1> | <0 0 1> | 68.0 |
C (mp-48) | <1 0 0> | <0 0 1> | 242.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 281.7 |
C (mp-48) | <1 1 0> | <0 0 1> | 233.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 184.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 272.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 242.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 145.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 204.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 97.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 136.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 340.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 116.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 233.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 233.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 233.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 242.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 68.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 272.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 68.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 97.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 233.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 48.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 116.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 174.9 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 184.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 155.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 272.0 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 242.9 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 242.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 310.9 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 301.2 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 223.4 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 126.3 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 340.0 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 242.9 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 272.0 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 310.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 272.0 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 204.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 194.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 126.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeMoS (mp-1027412) | 0.0798 | 0.077 | 3 |
TeMoS (mp-1027358) | 0.0824 | 0.078 | 3 |
TeWS (mp-1028761) | 0.0698 | 0.096 | 3 |
TeWS (mp-1028690) | 0.0774 | 0.096 | 3 |
TeWS (mp-1028526) | 0.0700 | 0.096 | 3 |
Te2MoWS2 (mp-1029072) | 0.0543 | 0.083 | 4 |
TeW2Se2S (mp-1028683) | 0.0510 | 0.050 | 4 |
Te2Mo3(SeS)2 (mp-1026002) | 0.0553 | 0.053 | 4 |
Te2W3(SeS)2 (mp-1025637) | 0.0237 | 0.065 | 4 |
TeMo2Se2S (mp-1027448) | 0.0402 | 0.040 | 4 |
WS2 (mp-1028441) | 0.3358 | 0.001 | 2 |
WSe2 (mp-1025572) | 0.3443 | 0.000 | 2 |
WS2 (mp-1025571) | 0.3366 | 0.001 | 2 |
WS2 (mp-1023925) | 0.3405 | 0.001 | 2 |
MoS2 (mp-1027525) | 0.3438 | 0.001 | 2 |
Te2Mo2W(SeS)2 (mp-1025956) | 0.0138 | 0.134 | 5 |
Te2MoW2(SeS)2 (mp-1025888) | 0.0155 | 0.136 | 5 |
Te2MoW2(SeS)2 (mp-1025856) | 0.0207 | 0.116 | 5 |
Te2Mo2W(SeS)2 (mp-1025778) | 0.0224 | 0.085 | 5 |
Te2MoW2(SeS)2 (mp-1025768) | 0.0233 | 0.088 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv Se S |
Final Energy/Atom-6.5616 eV |
Corrected Energy-60.3815 eV
-60.3815 eV = -59.0546 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)