Final Magnetic Moment0.016 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.661 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.105 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + WS2 + MoWSe4 + MoS2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 0 1> | <0 0 1> | 281.5 |
C (mp-48) | <1 1 0> | <0 0 1> | 233.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 116.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 242.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 233.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 242.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 242.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 145.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 203.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 97.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 135.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 339.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 271.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 68.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 97.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 116.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.1 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 174.7 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 184.4 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 223.3 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 126.2 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 242.7 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 300.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 126.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 271.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 203.9 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 145.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 38.8 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 116.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 320.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 68.0 |
BN (mp-984) | <1 1 1> | <0 0 1> | 262.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 48.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 116.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 29.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 223.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 262.1 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 310.6 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 310.6 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 213.6 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 77.7 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 126.2 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 330.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 68.0 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 126.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 378.6 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 155.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 106.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeMoS (mp-1027358) | 0.0579 | 0.078 | 3 |
TeWS (mp-1028761) | 0.0619 | 0.096 | 3 |
TeWS (mp-1028526) | 0.0474 | 0.097 | 3 |
TeMoS (mp-1027738) | 0.0459 | 0.078 | 3 |
TeWS (mp-1023931) | 0.0608 | 0.096 | 3 |
Te2MoWS2 (mp-1030196) | 0.0415 | 0.081 | 4 |
Te2MoWS2 (mp-1029946) | 0.0415 | 0.118 | 4 |
Te4MoW3S4 (mp-1028520) | 0.0431 | 0.088 | 4 |
Te2Mo3(SeS)2 (mp-1026002) | 0.0354 | 0.053 | 4 |
Te2W3(SeS)2 (mp-1025578) | 0.0352 | 0.066 | 4 |
WS2 (mp-1028441) | 0.3285 | 0.001 | 2 |
MoS2 (mp-1025874) | 0.3279 | 0.001 | 2 |
MoSe2 (mp-1025799) | 0.3288 | 0.000 | 2 |
MoSe2 (mp-1027692) | 0.3285 | 0.000 | 2 |
MoS2 (mp-1027525) | 0.3264 | 0.001 | 2 |
Te2Mo2W(SeS)2 (mp-1026027) | 0.0333 | 0.135 | 5 |
Te2Mo2W(SeS)2 (mp-1025933) | 0.0333 | 0.107 | 5 |
Te2MoW2(SeS)2 (mp-1025836) | 0.0334 | 0.137 | 5 |
Te2MoW2(SeS)2 (mp-1025722) | 0.0349 | 0.116 | 5 |
Te2Mo3W(Se2S)2 (mp-1027614) | 0.0380 | 0.102 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv Se S |
Final Energy/Atom-6.7583 eV |
Corrected Energy-62.1519 eV
-62.1519 eV = -60.8250 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)