material

ZnFe3C

ID:

mp-10266

DOI:

10.17188/1186863


Tags: Iron zinc carbide (3/1/1)

Material Details

Final Magnetic Moment
4.012 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
0.012 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.024 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.57 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Zn9Fe4 + C + Fe
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 76763 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Au (mp-81) <1 1 0> <1 1 0> 0.000 221.4
Ge (mp-32) <1 1 1> <1 1 1> 0.000 172.6
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.000 128.1
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 1 0> 0.002 161.0
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.002 113.9
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.002 355.9
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.003 227.8
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.007 128.1
InP (mp-20351) <1 0 0> <1 0 0> 0.008 71.2
BN (mp-984) <1 0 1> <1 1 1> 0.010 221.9
GaAs (mp-2534) <1 1 1> <1 1 1> 0.016 172.6
SiC (mp-11714) <1 0 0> <1 1 0> 0.020 281.8
Ag (mp-124) <1 1 0> <1 1 0> 0.021 221.4
SiC (mp-7631) <1 0 0> <1 1 0> 0.024 140.9
InAs (mp-20305) <1 1 0> <1 1 0> 0.036 161.0
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.038 113.9
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.042 172.6
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.046 227.8
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.049 161.0
Te2Mo (mp-602) <1 1 0> <1 1 0> 0.049 281.8
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.059 128.1
SiC (mp-11714) <0 0 1> <1 1 1> 0.062 24.7
ZnO (mp-2133) <1 1 0> <1 1 0> 0.066 60.4
SiC (mp-7631) <0 0 1> <1 1 1> 0.070 24.7
TePb (mp-19717) <1 1 1> <1 1 1> 0.075 74.0
TePb (mp-19717) <1 1 0> <1 1 0> 0.077 60.4
C (mp-66) <1 1 0> <1 1 0> 0.080 161.0
C (mp-66) <1 0 0> <1 0 0> 0.085 113.9
SiC (mp-8062) <1 1 1> <1 1 1> 0.091 98.6
SiC (mp-8062) <1 1 0> <1 1 0> 0.093 80.5
SiC (mp-7631) <1 1 0> <1 1 0> 0.100 80.5
SiC (mp-11714) <1 1 0> <1 1 0> 0.105 161.0
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.107 221.4
NaCl (mp-22862) <1 1 0> <1 1 0> 0.109 181.2
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.111 213.5
TiO2 (mp-2657) <1 0 0> <1 1 1> 0.114 221.9
NaCl (mp-22862) <1 0 0> <1 0 0> 0.115 128.1
PbS (mp-21276) <1 0 0> <1 0 0> 0.141 71.2
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.142 128.1
SiC (mp-11714) <1 0 1> <1 1 0> 0.153 161.0
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.159 161.0
GaTe (mp-542812) <1 0 -1> <1 1 0> 0.160 302.0
NdGaO3 (mp-3196) <1 0 1> <1 0 0> 0.162 213.5
Mg (mp-153) <0 0 1> <1 0 0> 0.169 156.6
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.176 181.2
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.186 128.1
SiC (mp-7631) <1 1 1> <1 0 0> 0.187 242.0
ZrO2 (mp-2858) <1 0 -1> <1 1 0> 0.189 181.2
SiC (mp-11714) <1 1 1> <1 1 0> 0.191 221.4
CdS (mp-672) <1 0 0> <1 1 0> 0.199 342.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
405 117 117 0 0 0
117 405 117 0 0 0
117 117 405 0 0 0
0 0 0 85 0 0
0 0 0 0 85 0
0 0 0 0 0 85
Compliance Tensor Sij (10-12Pa-1)
2.8 -0.6 -0.6 0 0 0
-0.6 2.8 -0.6 0 0 0
-0.6 -0.6 2.8 0 0 0
0 0 0 11.7 0 0
0 0 0 0 11.7 0
0 0 0 0 0 11.7
Shear Modulus GV
109 GPa
Bulk Modulus KV
213 GPa
Shear Modulus GR
102 GPa
Bulk Modulus KR
213 GPa
Shear Modulus GVRH
105 GPa
Bulk Modulus KVRH
213 GPa
Elastic Anisotropy
0.34
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sc3InC (mp-8578) 0.0000 0.000 3
TmBRh3 (mp-5438) 0.0000 0.000 3
Mn3ZnN (mp-15805) 0.0000 0.000 3
Sc3InB (mp-19726) 0.0000 0.085 3
Y3InC (mp-19817) 0.0000 0.000 3
Ba2VFeO6 (mp-1096778) 0.0000 2.272 4
Ba2ScSbO6 (mp-20709) 0.0000 2.196 4
Ba2YbSbO6 (mp-14223) 0.0000 1.746 4
Ba2YSbO6 (mp-14226) 0.0000 2.078 4
Ba2NbFeO6 (mp-1096853) 0.0000 2.945 4
Fe4N (mp-535) 0.0000 0.070 2
Sr3Sb2 (mp-1013583) 0.0000 0.378 2
Ni4N (mp-20839) 0.0000 2.019 2
Sr3P2 (mp-1013552) 0.0000 0.403 2
Ca3P2 (mp-1013547) 0.0000 0.146 2
BaLaMgBiO6 (mp-41414) 0.0488 0.096 5
BaLaMgNbO6 (mp-39288) 0.0712 0.090 5
SrLaNbZnO6 (mp-41918) 0.0665 0.126 5
SrLaMnCoO6 (mp-40761) 0.0404 0.253 5
Sr6Ca2MnFe7O24 (mp-1075969) 0.0482 0.021 5
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) 0.7380 0.065 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zn Fe_pv C
Final Energy/Atom
-7.1675 eV
Corrected Energy
-35.8377 eV
-35.8377 eV = -35.8377 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 76763
Submitted by
User remarks:
  • Iron zinc carbide (3/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)