Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.127 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.033 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToWS2 + MoWSe4 + MoS2 |
Band Gap0.796 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 35.9 |
C (mp-48) | <1 0 0> | <0 0 1> | 179.7 |
C (mp-48) | <1 0 1> | <0 0 1> | 179.7 |
C (mp-48) | <1 1 0> | <0 0 1> | 260.6 |
C (mp-48) | <1 1 1> | <0 0 1> | 206.7 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 170.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 224.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 9.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 143.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 206.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 143.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 206.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 89.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 125.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 170.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 287.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 287.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 278.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 62.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 143.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 314.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 143.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 314.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 287.5 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 179.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 224.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 161.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 305.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 53.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 323.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 188.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 62.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 161.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 323.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 170.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 80.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 161.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.0 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 314.5 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 251.6 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 62.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 251.6 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 278.5 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 206.7 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 287.5 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 350.4 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 287.5 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 251.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 215.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 179.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
WSeS (mp-1028764) | 0.0573 | 0.015 | 3 |
Mo3(SeS2)2 (mp-1025988) | 0.0378 | 0.014 | 3 |
W2SeS3 (mp-1028487) | 0.0197 | 0.011 | 3 |
W3(SeS2)2 (mp-1025577) | 0.0268 | 0.013 | 3 |
Mo2SeS3 (mp-1027608) | 0.0507 | 0.011 | 3 |
MoWSeS3 (mp-1030131) | 0.0101 | 0.051 | 4 |
Mo3W(SeS3)2 (mp-1027294) | 0.0081 | 0.033 | 4 |
MoW3(SeS3)2 (mp-1028917) | 0.0121 | 0.051 | 4 |
MoWSeS3 (mp-1026975) | 0.0089 | 0.033 | 4 |
MoWSeS3 (mp-1030745) | 0.0095 | 0.034 | 4 |
WSe2 (mp-1028698) | 0.1485 | 0.000 | 2 |
WS2 (mp-1028441) | 0.1337 | 0.001 | 2 |
WSe2 (mp-1025572) | 0.1480 | 0.000 | 2 |
WS2 (mp-1025571) | 0.1373 | 0.001 | 2 |
WS2 (mp-1023925) | 0.1509 | 0.001 | 2 |
Te4Mo3W(SeS)2 (mp-1030576) | 0.1784 | 0.082 | 5 |
Te4Mo3W(SeS)2 (mp-1030338) | 0.1756 | 0.097 | 5 |
Te2MoWSeS (mp-1030176) | 0.1695 | 0.083 | 5 |
Te2MoWSeS (mp-1028919) | 0.1789 | 0.119 | 5 |
Te4Mo3W(SeS)2 (mp-1027133) | 0.1772 | 0.116 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mo_pv W_pv Se S |
Final Energy/Atom-7.2373 eV |
Corrected Energy-90.8280 eV
-90.8280 eV = -86.8473 eV (uncorrected energy) - 3.9808 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)