Final Magnetic Moment0.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.613 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.141 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + WS2 + MoWSe4 |
Band Gap0.309 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 38.8 |
C (mp-48) | <1 0 0> | <0 0 1> | 281.1 |
C (mp-48) | <1 0 1> | <0 0 1> | 281.1 |
C (mp-48) | <1 1 0> | <0 0 1> | 232.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 184.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 116.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 242.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 232.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 242.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 164.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 339.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 155.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 232.6 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 232.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 242.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 271.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 67.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 67.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 242.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 145.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 203.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 67.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 96.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 135.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 339.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 271.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 67.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 96.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 232.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 242.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 48.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 116.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.1 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 174.5 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 184.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 155.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 271.4 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 242.3 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 222.9 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 242.3 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 126.0 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 339.2 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 242.3 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 271.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 310.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 310.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 300.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 126.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 271.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 271.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeMoS (mp-1027358) | 0.0894 | 0.078 | 3 |
TeWS (mp-1028761) | 0.0741 | 0.096 | 3 |
TeWS (mp-1028690) | 0.0824 | 0.097 | 3 |
TeWS (mp-1028526) | 0.0778 | 0.097 | 3 |
TeMoS (mp-1027738) | 0.0917 | 0.078 | 3 |
TeW2Se2S (mp-1028683) | 0.0190 | 0.050 | 4 |
Te2Mo3(SeS)2 (mp-1025927) | 0.0400 | 0.053 | 4 |
Te2W3(SeS)2 (mp-1025637) | 0.0331 | 0.066 | 4 |
TeMo2Se2S (mp-1027547) | 0.0549 | 0.040 | 4 |
TeMo2Se2S (mp-1027448) | 0.0182 | 0.040 | 4 |
WSe2 (mp-1028698) | 0.3484 | 0.000 | 2 |
WS2 (mp-1028441) | 0.3432 | 0.001 | 2 |
MoSe2 (mp-1027692) | 0.3508 | 0.000 | 2 |
WSe2 (mp-1025572) | 0.3498 | 0.000 | 2 |
WS2 (mp-1025571) | 0.3460 | 0.001 | 2 |
Te2Mo3W(Se2S)2 (mp-1027337) | 0.0135 | 0.102 | 5 |
TeMoWSe2S (mp-1027309) | 0.0149 | 0.120 | 5 |
TeMoWSe2S (mp-1027049) | 0.0032 | 0.141 | 5 |
Te2MoW3(Se2S)2 (mp-1027001) | 0.0035 | 0.128 | 5 |
Te2Mo3W(Se2S)2 (mp-1026941) | 0.0048 | 0.124 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv Se S |
Final Energy/Atom-6.8481 eV |
Corrected Energy-85.9154 eV
Uncorrected energy = -82.1774 eV
Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV
Composition-based energy adjustment (-0.472 eV/atom x 4.0 atoms) = -1.8880 eV
Composition-based energy adjustment (-0.422 eV/atom x 2.0 atoms) = -0.8440 eV
Corrected energy = -85.9154 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)