Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.928 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.098 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + WS2 + MoS2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 37.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 297.0 |
C (mp-48) | <1 0 1> | <0 0 1> | 157.8 |
C (mp-48) | <1 1 0> | <0 0 1> | 222.7 |
C (mp-48) | <1 1 1> | <0 0 1> | 343.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 176.3 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 232.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 111.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 250.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 259.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 371.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 148.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 167.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 315.6 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 176.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 194.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 204.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 139.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 324.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 297.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 297.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 287.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 92.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 362.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 222.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 194.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 167.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 315.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 176.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 176.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 111.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.8 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 324.8 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 250.6 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 65.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 213.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 259.9 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 213.5 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 232.0 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 120.7 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 222.7 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 297.0 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 259.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 297.0 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 185.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Te2Mo3S4 (mp-1026020) | 0.1047 | 0.070 | 3 |
Te2Mo3S4 (mp-1025986) | 0.0748 | 0.069 | 3 |
Te2W3S4 (mp-1025690) | 0.0591 | 0.083 | 3 |
TeMo2S3 (mp-1027696) | 0.0190 | 0.059 | 3 |
Te2W3S4 (mp-1025586) | 0.0976 | 0.082 | 3 |
Te2Mo(WS2)3 (mp-1029076) | 0.0084 | 0.099 | 4 |
Te2Mo(WS2)3 (mp-1028999) | 0.0228 | 0.062 | 4 |
Te2Mo3WS6 (mp-1027706) | 0.0179 | 0.060 | 4 |
Te2Mo3WS6 (mp-1027567) | 0.0487 | 0.059 | 4 |
TeMoWS3 (mp-1080160) | 0.0142 | 0.099 | 4 |
WSe2 (mp-1028698) | 0.3777 | 0.000 | 2 |
WSe2 (mp-1025572) | 0.3768 | 0.000 | 2 |
Te2W (mp-1023942) | 0.3742 | 0.026 | 2 |
Te2Mo (mp-1023938) | 0.3763 | 0.001 | 2 |
WSe2 (mp-1023933) | 0.3767 | 0.001 | 2 |
Te2MoW3(SeS2)2 (mp-1030569) | 0.0629 | 0.100 | 5 |
TeMoWSeS2 (mp-1027050) | 0.0677 | 0.114 | 5 |
TeMoWSeS2 (mp-1027740) | 0.0682 | 0.114 | 5 |
Te2Mo3W(SeS2)2 (mp-1027570) | 0.0684 | 0.114 | 5 |
TeMoWSeS2 (mp-1080161) | 0.0659 | 0.115 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv S |
Final Energy/Atom-7.1561 eV |
Corrected Energy-89.7357 eV
Uncorrected energy = -85.8737 eV
Composition-based energy adjustment (-0.503 eV/atom x 6.0 atoms) = -3.0180 eV
Composition-based energy adjustment (-0.422 eV/atom x 2.0 atoms) = -0.8440 eV
Corrected energy = -89.7357 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)