material

ZnCo3C

ID:

mp-10271

DOI:

10.17188/1186867


Tags: Cobalt zinc carbide (3/1/1)

Material Details

Final Magnetic Moment
1.044 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.018 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.004 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.08 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Zn11Co2 + C + Co
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 76797 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
PbSe (mp-2201) <1 0 0> <1 0 0> 0.001 349.3
GaSb (mp-1156) <1 0 0> <1 0 0> 0.011 349.3
Au (mp-81) <1 0 0> <1 0 0> 0.012 69.9
GaN (mp-804) <1 0 1> <1 0 0> 0.021 209.6
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.025 251.5
CdSe (mp-2691) <1 0 0> <1 0 0> 0.026 349.3
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.026 55.9
NaCl (mp-22862) <1 1 1> <1 1 1> 0.032 169.4
Mg (mp-153) <1 0 0> <1 0 0> 0.042 83.8
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.050 177.8
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.050 209.6
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.057 316.2
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.059 125.7
Ni (mp-23) <1 1 0> <1 1 0> 0.069 158.1
Ag (mp-124) <1 0 0> <1 0 0> 0.069 69.9
Ni (mp-23) <1 0 0> <1 0 0> 0.073 111.8
SiO2 (mp-6930) <1 1 1> <1 1 0> 0.076 158.1
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.082 177.8
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.089 125.7
TbScO3 (mp-31119) <1 0 1> <1 1 0> 0.094 335.9
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.105 169.4
LaF3 (mp-905) <0 0 1> <1 1 1> 0.113 314.6
Ga2O3 (mp-886) <1 0 1> <1 1 0> 0.115 138.3
GdScO3 (mp-5690) <1 0 1> <1 1 0> 0.117 335.9
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.124 125.7
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.127 48.4
DyScO3 (mp-31120) <1 0 1> <1 1 0> 0.136 335.9
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 0.140 223.6
Ag (mp-124) <1 1 0> <1 1 0> 0.153 217.4
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.160 223.6
GaAs (mp-2534) <1 1 1> <1 1 1> 0.162 169.4
Cu (mp-30) <1 1 1> <1 0 0> 0.165 251.5
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.167 27.9
CdWO4 (mp-19387) <0 1 0> <1 1 1> 0.168 290.4
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.170 125.7
Mg (mp-153) <1 0 1> <1 0 0> 0.178 209.6
GaN (mp-804) <1 0 0> <1 0 0> 0.179 83.8
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.180 355.7
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.182 111.8
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.185 39.5
GaN (mp-804) <1 1 0> <1 1 0> 0.187 59.3
C (mp-48) <0 0 1> <1 1 0> 0.191 79.0
SiC (mp-11714) <1 1 1> <1 1 0> 0.207 217.4
BN (mp-984) <1 0 1> <1 1 1> 0.216 217.8
InP (mp-20351) <1 0 0> <1 0 0> 0.220 69.9
Te2Mo (mp-602) <1 0 1> <1 1 0> 0.229 276.6
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.229 314.6
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.237 276.6
CdS (mp-672) <1 0 1> <1 0 0> 0.243 321.4
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 1 0> 0.244 158.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
428 111 111 0 0 0
111 428 111 0 0 0
111 111 428 0 0 0
0 0 0 90 0 0
0 0 0 0 90 0
0 0 0 0 0 90
Compliance Tensor Sij (10-12Pa-1)
2.6 -0.5 -0.5 0 0 0
-0.5 2.6 -0.5 0 0 0
-0.5 -0.5 2.6 0 0 0
0 0 0 11.1 0 0
0 0 0 0 11.1 0
0 0 0 0 0 11.1
Shear Modulus GV
117 GPa
Bulk Modulus KV
217 GPa
Shear Modulus GR
109 GPa
Bulk Modulus KR
217 GPa
Shear Modulus GVRH
113 GPa
Bulk Modulus KVRH
217 GPa
Elastic Anisotropy
0.39
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LuBPd3 (mp-3105) 0.0000 0.111 3
Mn3NiN (mp-20362) 0.0000 0.060 3
LaBPd3 (mp-3846) 0.0000 0.138 3
Lu3TlC (mp-10607) 0.0000 0.000 3
YbRh3C (mp-10716) 0.0000 0.000 3
Ba2VFeO6 (mp-1096778) 0.0000 2.272 4
Ba2ScSbO6 (mp-20709) 0.0000 2.196 4
Ba2YbSbO6 (mp-14223) 0.0000 1.747 4
Ba2YSbO6 (mp-14226) 0.0000 2.082 4
Ba2NbFeO6 (mp-1096853) 0.0000 2.749 4
Ba3Sb2 (mp-1013582) 0.0000 0.409 2
Ca3Bi2 (mp-1013735) 0.0000 0.366 2
Ba3N2 (mp-1013528) 0.0000 0.683 2
Ba3P2 (mp-1013551) 0.0000 0.446 2
Sr3Bi2 (mp-1013587) 0.0000 0.373 2
BaLaMgBiO6 (mp-41414) 0.0488 0.096 5
BaLaMgNbO6 (mp-39288) 0.0712 0.090 5
SrLaNbZnO6 (mp-41918) 0.0665 0.126 5
SrLaMnCoO6 (mp-40761) 0.0404 0.247 5
Sr6Ca2MnFe7O24 (mp-1075969) 0.0482 0.021 5
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) 0.7380 0.065 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zn Co C
Final Energy/Atom
-6.3800 eV
Corrected Energy
-31.8999 eV
Uncorrected energy = -31.8999 eV Corrected energy = -31.8999 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 76797
Submitted by
User remarks:
  • Cobalt zinc carbide (3/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)