Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.948 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.076 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoWSe4 + MoS2 |
Band Gap0.600 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 36.7 |
C (mp-48) | <1 0 0> | <0 0 1> | 293.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 183.7 |
C (mp-48) | <1 1 0> | <0 0 1> | 266.3 |
C (mp-48) | <1 1 1> | <0 0 1> | 321.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 174.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 229.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 110.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 248.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 257.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 257.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 367.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 146.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 165.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 312.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 174.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 321.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 284.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 202.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 137.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 146.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 321.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 293.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 293.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 284.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 91.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 358.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 220.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 192.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 165.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 312.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 174.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 82.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 110.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 321.4 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 248.0 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 64.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 211.2 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 293.9 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 229.6 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 211.2 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 275.5 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 119.4 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 358.2 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 293.9 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 257.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mo3(Se2S)2 (mp-1025906) | 0.1556 | 0.013 | 3 |
Mo2SeS3 (mp-1027890) | 0.1142 | 0.010 | 3 |
W3(Se2S)2 (mp-1025599) | 0.1560 | 0.013 | 3 |
MoWS4 (mp-1027647) | 0.1605 | 0.002 | 3 |
MoSeS (mp-1027580) | 0.1582 | 0.014 | 3 |
MoWSeS3 (mp-1030146) | 0.1329 | 0.034 | 4 |
MoW3(SeS)4 (mp-1028930) | 0.0249 | 0.077 | 4 |
MoW(SeS)2 (mp-1028832) | 0.1307 | 0.093 | 4 |
MoW2(SeS2)2 (mp-1025716) | 0.0641 | 0.066 | 4 |
Mo3W(SeS3)2 (mp-1027641) | 0.0692 | 0.051 | 4 |
WS2 (mp-1028441) | 0.2179 | 0.001 | 2 |
MoS2 (mp-1025874) | 0.2328 | 0.001 | 2 |
WS2 (mp-1025571) | 0.2176 | 0.001 | 2 |
WS2 (mp-1023925) | 0.2227 | 0.001 | 2 |
MoS2 (mp-1027525) | 0.2338 | 0.001 | 2 |
Te4Mo3W(SeS)2 (mp-1030576) | 0.2448 | 0.082 | 5 |
Te4Mo3W(SeS)2 (mp-1030338) | 0.2416 | 0.096 | 5 |
Te2MoWSeS (mp-1030176) | 0.2422 | 0.083 | 5 |
TeMoWSe2S (mp-1029116) | 0.2452 | 0.104 | 5 |
Te4Mo3W(SeS)2 (mp-1030753) | 0.1787 | 0.116 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mo_pv W_pv Se S |
Final Energy/Atom-7.0622 eV |
Corrected Energy-87.4005 eV
-87.4005 eV = -84.7467 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)