Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.916 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.099 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.27 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + WS2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 37.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 296.7 |
C (mp-48) | <1 0 1> | <0 0 1> | 157.6 |
C (mp-48) | <1 1 0> | <0 0 1> | 222.5 |
C (mp-48) | <1 1 1> | <0 0 1> | 343.1 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 176.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 231.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 111.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 250.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 259.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 370.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 148.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 166.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 315.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 176.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 194.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 64.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 204.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 139.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 324.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 296.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 296.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 287.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 92.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 361.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 222.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 194.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 166.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 315.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 176.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 176.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 111.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.8 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 324.5 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 250.3 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 64.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 213.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 259.6 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 213.2 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 231.8 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 120.5 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 222.5 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 296.7 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 259.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 296.7 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 185.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Te2Mo3S4 (mp-1026020) | 0.0752 | 0.070 | 3 |
TeW2S3 (mp-1028492) | 0.0134 | 0.069 | 3 |
TeMo2S3 (mp-1027761) | 0.0235 | 0.059 | 3 |
TeMo2S3 (mp-1027696) | 0.1089 | 0.059 | 3 |
Te2W3S4 (mp-1025586) | 0.0598 | 0.082 | 3 |
TeMoWS3 (mp-1030236) | 0.0128 | 0.098 | 4 |
Te2Mo(WS2)3 (mp-1029248) | 0.0092 | 0.099 | 4 |
TeMoWS3 (mp-1027303) | 0.0168 | 0.060 | 4 |
Te2Mo(WS2)3 (mp-1028929) | 0.0101 | 0.098 | 4 |
TeMoWS3 (mp-1027652) | 0.0080 | 0.099 | 4 |
MoSe2 (mp-1025799) | 0.3752 | 0.000 | 2 |
MoSe2 (mp-1027692) | 0.3751 | 0.000 | 2 |
WSe2 (mp-1025572) | 0.3793 | 0.000 | 2 |
MoSe2 (mp-1023940) | 0.3762 | 0.000 | 2 |
WSe2 (mp-1023933) | 0.3793 | 0.001 | 2 |
Te2MoW3(SeS2)2 (mp-1030244) | 0.0667 | 0.099 | 5 |
TeMoWSeS2 (mp-1029063) | 0.0687 | 0.114 | 5 |
Te2MoW3(SeS2)2 (mp-1029044) | 0.0662 | 0.100 | 5 |
Te2MoW3(SeS2)2 (mp-1028490) | 0.0677 | 0.101 | 5 |
TeMoWSeS2 (mp-1029282) | 0.0683 | 0.114 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv S |
Final Energy/Atom-7.3192 eV |
Corrected Energy-91.8116 eV
-91.8116 eV = -87.8308 eV (uncorrected energy) - 3.9808 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)