Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.124 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToWS2 + MoSe2 + MoS2 |
Band Gap0.535 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 36.0 |
C (mp-48) | <1 0 0> | <0 0 1> | 180.0 |
C (mp-48) | <1 0 1> | <0 0 1> | 180.0 |
C (mp-48) | <1 1 0> | <0 0 1> | 261.0 |
C (mp-48) | <1 1 1> | <0 0 1> | 207.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 171.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 225.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 9.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 144.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 207.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 144.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 207.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 90.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 126.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 162.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 234.0 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 171.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 288.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 288.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 279.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 63.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 144.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 315.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 144.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 315.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 288.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 180.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 225.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 90.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 306.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 54.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 306.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 54.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 189.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 63.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 162.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 324.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 171.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 81.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 162.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.0 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 315.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 252.0 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 63.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 252.0 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 279.0 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 207.0 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 270.0 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 351.0 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 288.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
WSeS (mp-1028764) | 0.0490 | 0.015 | 3 |
WSeS (mp-1028488) | 0.0466 | 0.015 | 3 |
Mo3(SeS2)2 (mp-1025925) | 0.0298 | 0.013 | 3 |
W3(SeS2)2 (mp-1025584) | 0.0280 | 0.013 | 3 |
Mo2SeS3 (mp-1027608) | 0.0040 | 0.011 | 3 |
MoWSeS3 (mp-1027391) | 0.0071 | 0.011 | 4 |
MoWSeS3 (mp-1027292) | 0.0080 | 0.011 | 4 |
MoWSeS3 (mp-1027143) | 0.0090 | 0.028 | 4 |
Mo3W(SeS3)2 (mp-1027646) | 0.0031 | 0.011 | 4 |
Mo3W(SeS3)2 (mp-1027472) | 0.0059 | 0.011 | 4 |
Te2Mo (mp-1030319) | 0.1601 | 0.001 | 2 |
WS2 (mp-1028441) | 0.1475 | 0.001 | 2 |
Te2Mo (mp-1025576) | 0.1584 | 0.002 | 2 |
WS2 (mp-1025571) | 0.1502 | 0.001 | 2 |
Te2Mo (mp-1023938) | 0.1594 | 0.002 | 2 |
Te4Mo3W(SeS)2 (mp-1030576) | 0.1904 | 0.060 | 5 |
Te4Mo3W(SeS)2 (mp-1030338) | 0.1860 | 0.075 | 5 |
Te4Mo3W(SeS)2 (mp-1030252) | 0.1925 | 0.074 | 5 |
Te2MoWSeS (mp-1030176) | 0.1861 | 0.060 | 5 |
Te2MoWSeS (mp-1029121) | 0.1919 | 0.060 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mo_pv W_pv Se S |
Final Energy/Atom-7.2350 eV |
Corrected Energy-90.8011 eV
-90.8011 eV = -86.8204 eV (uncorrected energy) - 3.9808 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)