Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.177 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.042 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2W + WSe2 |
Band Gap1.278 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 127.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 169.5 |
C (mp-48) | <1 0 1> | <0 0 1> | 296.6 |
C (mp-48) | <1 1 0> | <0 0 1> | 328.4 |
C (mp-48) | <1 1 1> | <0 0 1> | 307.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 74.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 74.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 233.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 127.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 328.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 180.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 264.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 286.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 201.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 169.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 201.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 201.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 286.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 254.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 286.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 74.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 296.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 349.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 190.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 201.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 169.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 201.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 211.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 201.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 105.9 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 254.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 296.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 275.4 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 296.6 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 211.9 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 233.1 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 307.2 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 275.4 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 317.8 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 116.5 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 328.4 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 296.6 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 74.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 10.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 275.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 286.0 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 275.4 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 95.3 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 84.7 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 84.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
W2Se3S (mp-1028769) | 0.0715 | 0.011 | 3 |
Te4W3Se2 (mp-1026350) | 0.0512 | 0.044 | 3 |
Te4Mo3Se2 (mp-1025733) | 0.0459 | 0.025 | 3 |
Te3Mo2Se (mp-1030721) | 0.0192 | 0.021 | 3 |
Mo2Se3S (mp-1027483) | 0.0837 | 0.011 | 3 |
Te6MoW3Se2 (mp-1030107) | 0.0065 | 0.060 | 4 |
Te3MoWSe (mp-1028843) | 0.0064 | 0.053 | 4 |
Te6MoW3Se2 (mp-1028646) | 0.0038 | 0.060 | 4 |
Te6MoW3Se2 (mp-1028433) | 0.0060 | 0.060 | 4 |
Te3MoWSe (mp-1029284) | 0.0076 | 0.053 | 4 |
Te2Mo (mp-1030319) | 0.2501 | 0.000 | 2 |
WS2 (mp-1028441) | 0.2347 | 0.001 | 2 |
WS2 (mp-1025571) | 0.2402 | 0.001 | 2 |
WS2 (mp-1023925) | 0.2519 | 0.001 | 2 |
NbSe2 (mp-568347) | 0.2512 | 0.007 | 2 |
TeMoWSe2S (mp-1029116) | 0.1433 | 0.104 | 5 |
TeMoWSe2S (mp-1028959) | 0.1455 | 0.104 | 5 |
TeMoWSe2S (mp-1028939) | 0.1452 | 0.104 | 5 |
TeMoWSe2S (mp-1027138) | 0.1446 | 0.120 | 5 |
Te2Mo3W(Se2S)2 (mp-1030827) | 0.1413 | 0.087 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te W_pv Se |
Final Energy/Atom-6.6505 eV |
Corrected Energy-79.8057 eV
-79.8057 eV = -79.8057 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)