Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.432 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.075 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2W + WSe2 + WS2 |
Band Gap0.287 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 70.0 |
C (mp-48) | <1 0 0> | <0 0 1> | 249.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 289.8 |
C (mp-48) | <1 1 0> | <0 0 1> | 239.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 309.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 129.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 249.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 189.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 189.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 169.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 349.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 349.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 159.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 99.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 139.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 349.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 279.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 70.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 90.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 249.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 249.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 279.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 70.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 159.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 139.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 279.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 349.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 269.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 70.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 99.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 139.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 179.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 199.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 189.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 179.9 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 189.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 131.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 159.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 279.8 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 279.8 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 249.9 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 249.9 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 129.9 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 219.9 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 249.9 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 309.8 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 349.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 309.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 129.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 279.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeMoS (mp-1030461) | 0.0673 | 0.078 | 3 |
Te3W2S (mp-1028755) | 0.0860 | 0.083 | 3 |
TeWS (mp-1028604) | 0.0747 | 0.097 | 3 |
Te4W3S2 (mp-1026362) | 0.0494 | 0.092 | 3 |
Te4Mo3S2 (mp-1025769) | 0.0634 | 0.070 | 3 |
Te2Mo2SeS (mp-1030459) | 0.0165 | 0.055 | 4 |
Te4Mo3WS4 (mp-1030269) | 0.0660 | 0.080 | 4 |
Te4Mo(WS)2 (mp-1026352) | 0.0553 | 0.129 | 4 |
Te4Mo(WS)2 (mp-1025710) | 0.0484 | 0.083 | 4 |
Te4Mo2WS2 (mp-1025654) | 0.0601 | 0.074 | 4 |
WSe2 (mp-1028698) | 0.2927 | 0.000 | 2 |
WS2 (mp-1028441) | 0.2966 | 0.001 | 2 |
MoSe2 (mp-1025799) | 0.2921 | 0.000 | 2 |
MoSe2 (mp-1027692) | 0.2911 | 0.000 | 2 |
WSe2 (mp-1025572) | 0.2927 | 0.000 | 2 |
Te2MoWSeS (mp-1030392) | 0.0060 | 0.105 | 5 |
Te4MoW3(SeS)2 (mp-1029233) | 0.0085 | 0.092 | 5 |
Te2MoWSeS (mp-1029154) | 0.0077 | 0.104 | 5 |
Te4MoW3(SeS)2 (mp-1028626) | 0.0042 | 0.111 | 5 |
Te2MoWSeS (mp-1029379) | 0.0079 | 0.119 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te W_pv Se S |
Final Energy/Atom-6.9610 eV |
Corrected Energy-87.1696 eV
Uncorrected energy = -83.5316 eV
Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV
Composition-based energy adjustment (-0.472 eV/atom x 2.0 atoms) = -0.9440 eV
Composition-based energy adjustment (-0.422 eV/atom x 4.0 atoms) = -1.6880 eV
Corrected energy = -87.1696 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)