Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.483 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.091 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + Te2W + WS2 + MoWSe4 |
Band Gap0.611 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 69.9 |
C (mp-48) | <1 0 0> | <0 0 1> | 249.5 |
C (mp-48) | <1 0 1> | <0 0 1> | 289.4 |
C (mp-48) | <1 1 0> | <0 0 1> | 239.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 309.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 129.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 249.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 189.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 189.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 169.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 349.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 349.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 159.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 99.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 139.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 349.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 279.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 69.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 89.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 249.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 249.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 209.6 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 279.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 69.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 159.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 139.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 279.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 349.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 269.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 69.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 99.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 139.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 179.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 199.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 189.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 179.6 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 189.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 229.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 279.4 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 279.4 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 249.5 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 249.5 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 129.7 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 219.5 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 249.5 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 309.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 349.3 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 309.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 129.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 279.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeMoS (mp-1027358) | 0.0880 | 0.078 | 3 |
TeWS (mp-1028761) | 0.0821 | 0.096 | 3 |
TeWS (mp-1028526) | 0.1014 | 0.096 | 3 |
Te4Mo3S2 (mp-1025937) | 0.0959 | 0.071 | 3 |
Te4W3S2 (mp-1025587) | 0.0856 | 0.093 | 3 |
Te2MoWS2 (mp-1029072) | 0.0769 | 0.083 | 4 |
Te2W2SeS (mp-1028912) | 0.0234 | 0.074 | 4 |
Te2W2SeS (mp-1028771) | 0.0675 | 0.074 | 4 |
Te2W2SeS (mp-1028679) | 0.0795 | 0.073 | 4 |
Te2Mo3(SeS)2 (mp-1025927) | 0.0770 | 0.053 | 4 |
Te2Mo (mp-1030319) | 0.3674 | 0.000 | 2 |
WSe2 (mp-1028698) | 0.3662 | 0.000 | 2 |
Te2W (mp-1028586) | 0.3676 | 0.025 | 2 |
WS2 (mp-1028441) | 0.3620 | 0.001 | 2 |
WS2 (mp-1025571) | 0.3651 | 0.001 | 2 |
Te2MoWSeS (mp-1027372) | 0.0519 | 0.119 | 5 |
Te4Mo3W(SeS)2 (mp-1027053) | 0.0217 | 0.116 | 5 |
Te2MoWSeS (mp-1027015) | 0.0183 | 0.140 | 5 |
Te2MoWSeS (mp-1030700) | 0.0087 | 0.104 | 5 |
Te4MoW3(SeS)2 (mp-1080237) | 0.0152 | 0.127 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv Se S |
Final Energy/Atom-6.8357 eV |
Corrected Energy-83.3548 eV
-83.3548 eV = -82.0279 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)