Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.318 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.104 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.10 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2W + MoWSe4 |
Band Gap0.806 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 71.7 |
C (mp-48) | <1 0 0> | <0 0 1> | 256.2 |
C (mp-48) | <1 0 1> | <0 0 1> | 338.2 |
C (mp-48) | <1 1 0> | <0 0 1> | 317.7 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 71.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 133.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 256.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 276.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 174.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 235.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 164.0 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 164.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 358.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 276.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 71.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 92.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 194.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 276.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 286.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 71.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 286.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 338.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 194.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 164.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 184.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 204.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 194.7 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 245.9 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 245.9 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 194.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 134.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 164.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 286.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 266.4 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 317.7 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 256.2 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 225.4 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 235.7 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 317.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 215.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 71.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 133.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 286.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 276.7 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 286.9 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 61.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 123.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 194.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 71.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeWSe (mp-1028749) | 0.0440 | 0.043 | 3 |
Te4W3Se2 (mp-1026350) | 0.0598 | 0.044 | 3 |
TeWSe (mp-1028456) | 0.0142 | 0.043 | 3 |
TeMoSe (mp-1027683) | 0.0355 | 0.029 | 3 |
TeMoSe (mp-1030732) | 0.0142 | 0.028 | 3 |
Te2MoWSe2 (mp-1030613) | 0.0070 | 0.098 | 4 |
Te2MoWSe2 (mp-1030292) | 0.0071 | 0.097 | 4 |
Te4MoW3Se4 (mp-1029101) | 0.0054 | 0.105 | 4 |
Te2MoWSe2 (mp-1028828) | 0.0048 | 0.098 | 4 |
Te4Mo3WSe4 (mp-1030736) | 0.0089 | 0.111 | 4 |
WSe2 (mp-1028698) | 0.2004 | 0.000 | 2 |
WS2 (mp-1028441) | 0.2024 | 0.001 | 2 |
MoSe2 (mp-1027692) | 0.2061 | 0.000 | 2 |
WSe2 (mp-1025572) | 0.2034 | 0.000 | 2 |
WS2 (mp-1025571) | 0.2077 | 0.001 | 2 |
Te4Mo3W(SeS)2 (mp-1030576) | 0.1290 | 0.082 | 5 |
Te4Mo3W(SeS)2 (mp-1030338) | 0.1257 | 0.097 | 5 |
Te2MoWSeS (mp-1030176) | 0.1216 | 0.083 | 5 |
Te2MoWSeS (mp-1029121) | 0.1300 | 0.084 | 5 |
Te2MoWSeS (mp-1028919) | 0.1304 | 0.119 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv Se |
Final Energy/Atom-6.6748 eV |
Corrected Energy-80.0980 eV
-80.0980 eV = -80.0980 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)