Final Magnetic Moment0.006 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.747 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.116 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + Te2W + WS2 + MoWSe4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 37.9 |
C (mp-48) | <1 0 0> | <0 0 1> | 312.8 |
C (mp-48) | <1 0 1> | <0 0 1> | 161.2 |
C (mp-48) | <1 1 0> | <0 0 1> | 227.5 |
C (mp-48) | <1 1 1> | <0 0 1> | 350.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 180.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 237.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 113.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 256.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 227.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 218.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 331.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 331.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 151.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 227.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 227.5 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 180.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 199.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 66.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 66.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 303.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 142.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 331.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 293.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 94.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 227.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 56.9 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 265.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 66.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 227.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 227.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 180.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 47.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 113.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 28.4 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 256.0 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 180.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 151.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 265.4 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 265.4 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 218.0 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 237.0 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 123.2 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 237.0 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 265.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 303.4 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 189.6 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 237.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 180.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 265.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Te2Mo3S4 (mp-1026020) | 0.0786 | 0.070 | 3 |
Te2Mo3S4 (mp-1025986) | 0.0564 | 0.069 | 3 |
Te2W3S4 (mp-1025690) | 0.0549 | 0.083 | 3 |
TeMo2S3 (mp-1027696) | 0.0581 | 0.059 | 3 |
Te2W3S4 (mp-1025586) | 0.0810 | 0.082 | 3 |
TeW2SeS2 (mp-1028793) | 0.0440 | 0.064 | 4 |
TeW2SeS2 (mp-1028710) | 0.0102 | 0.062 | 4 |
Te2Mo2WS4 (mp-1025932) | 0.0519 | 0.071 | 4 |
Te2Mo(WS2)2 (mp-1025851) | 0.0542 | 0.122 | 4 |
TeMo2SeS2 (mp-1027471) | 0.0204 | 0.052 | 4 |
WSe2 (mp-1028698) | 0.3580 | 0.000 | 2 |
WS2 (mp-1028441) | 0.3558 | 0.001 | 2 |
MoSe2 (mp-1027692) | 0.3589 | 0.000 | 2 |
WSe2 (mp-1025572) | 0.3582 | 0.000 | 2 |
WS2 (mp-1025571) | 0.3575 | 0.001 | 2 |
Te2Mo3W(SeS2)2 (mp-1027095) | 0.0097 | 0.113 | 5 |
TeMoWSeS2 (mp-1027050) | 0.0068 | 0.114 | 5 |
TeMoWSeS2 (mp-1026988) | 0.0094 | 0.130 | 5 |
Te2MoW3(SeS2)2 (mp-1026930) | 0.0056 | 0.116 | 5 |
TeMoWSeS2 (mp-1027740) | 0.0069 | 0.114 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv Se S |
Final Energy/Atom-7.1547 eV |
Corrected Energy-89.6563 eV
Uncorrected energy = -85.8563 eV
Composition-based energy adjustment (-0.503 eV/atom x 4.0 atoms) = -2.0120 eV
Composition-based energy adjustment (-0.472 eV/atom x 2.0 atoms) = -0.9440 eV
Composition-based energy adjustment (-0.422 eV/atom x 2.0 atoms) = -0.8440 eV
Corrected energy = -89.6563 eV
|