Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.572 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.049 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2W + WSe2 + WS2 |
Band Gap0.622 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 38.7 |
C (mp-48) | <1 0 0> | <0 0 1> | 280.7 |
C (mp-48) | <1 0 1> | <0 0 1> | 280.7 |
C (mp-48) | <1 1 0> | <0 0 1> | 232.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 183.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 116.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 242.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 232.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 242.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 164.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 338.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 154.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 232.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 232.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 242.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 271.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 67.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 67.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 242.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 145.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 203.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 67.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 96.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 135.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 338.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 271.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 67.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 232.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 232.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 242.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 48.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 116.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.0 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 174.3 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 183.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 154.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 271.1 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 242.0 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 222.7 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 242.0 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 125.8 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 338.8 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 242.0 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 271.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 309.8 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 309.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 300.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 125.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 271.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 271.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeMoS (mp-1027358) | 0.1224 | 0.078 | 3 |
TeWS (mp-1028526) | 0.1230 | 0.097 | 3 |
TeMo2S3 (mp-1027761) | 0.1290 | 0.059 | 3 |
TeMoS (mp-1027738) | 0.1131 | 0.078 | 3 |
Te2W3S4 (mp-1025586) | 0.1289 | 0.082 | 3 |
Te4Mo3WS4 (mp-1030354) | 0.0673 | 0.079 | 4 |
Te4MoW3S4 (mp-1030153) | 0.0583 | 0.089 | 4 |
Te2MoWS2 (mp-1029950) | 0.0898 | 0.118 | 4 |
Te4MoW3S4 (mp-1027169) | 0.0865 | 0.125 | 4 |
TeMo2Se2S (mp-1027576) | 0.0352 | 0.040 | 4 |
WSe2 (mp-1028698) | 0.3250 | 0.000 | 2 |
MoSe2 (mp-1025799) | 0.3180 | 0.000 | 2 |
MoSe2 (mp-1027692) | 0.3160 | 0.000 | 2 |
MoSe2 (mp-1023940) | 0.3222 | 0.000 | 2 |
MoS2 (mp-1027525) | 0.3225 | 0.001 | 2 |
Te2MoW3(Se2S)2 (mp-1029951) | 0.0604 | 0.090 | 5 |
TeMoWSe2S (mp-1027526) | 0.0687 | 0.140 | 5 |
Te2Mo3W(Se2S)2 (mp-1027517) | 0.0590 | 0.102 | 5 |
TeMoWSe2S (mp-1030685) | 0.0704 | 0.103 | 5 |
Te2Mo3W(Se2S)2 (mp-1027512) | 0.0619 | 0.124 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te W_pv Se S |
Final Energy/Atom-7.1593 eV |
Corrected Energy-87.2389 eV
-87.2389 eV = -85.9120 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)