Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.637 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.089 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + Te2W + WS2 |
Band Gap0.343 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 68.3 |
C (mp-48) | <1 0 0> | <0 0 1> | 243.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 283.0 |
C (mp-48) | <1 1 0> | <0 0 1> | 234.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 185.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 117.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 243.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 234.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 243.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 165.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 341.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 156.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 97.6 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 234.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 273.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 68.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 243.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 243.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 204.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 97.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 136.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 273.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 341.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 273.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 68.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 97.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 234.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 48.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 117.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 175.6 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 185.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 156.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 273.2 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 243.9 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 243.9 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 243.9 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 126.8 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 341.5 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 243.9 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 273.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 312.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 312.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 302.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 126.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 273.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 273.2 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 204.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeMoS (mp-1027412) | 0.0373 | 0.078 | 3 |
TeWS (mp-1028761) | 0.0550 | 0.096 | 3 |
TeWS (mp-1028690) | 0.0099 | 0.097 | 3 |
TeWS (mp-1028526) | 0.0321 | 0.097 | 3 |
TeMoS (mp-1027738) | 0.0513 | 0.078 | 3 |
Te2MoWS2 (mp-1030398) | 0.0167 | 0.081 | 4 |
Te2MoWS2 (mp-1030309) | 0.0122 | 0.118 | 4 |
Te4Mo3WS4 (mp-1030240) | 0.0170 | 0.079 | 4 |
Te4MoW3S4 (mp-1029235) | 0.0047 | 0.090 | 4 |
Te2MoWS2 (mp-1028975) | 0.0117 | 0.117 | 4 |
WS2 (mp-1028441) | 0.3473 | 0.001 | 2 |
MoS2 (mp-1025874) | 0.3486 | 0.001 | 2 |
MoSe2 (mp-1025799) | 0.3498 | 0.000 | 2 |
MoSe2 (mp-1027692) | 0.3482 | 0.000 | 2 |
MoS2 (mp-1027525) | 0.3454 | 0.001 | 2 |
Te2Mo2W(SeS)2 (mp-1026027) | 0.0528 | 0.135 | 5 |
Te2Mo2W(SeS)2 (mp-1025933) | 0.0547 | 0.107 | 5 |
Te2MoW2(SeS)2 (mp-1025836) | 0.0522 | 0.137 | 5 |
Te2Mo2W(SeS)2 (mp-1025772) | 0.0555 | 0.086 | 5 |
Te2MoW2(SeS)2 (mp-1025722) | 0.0529 | 0.116 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv S |
Final Energy/Atom-6.9853 eV |
Corrected Energy-87.5232 eV
Uncorrected energy = -83.8232 eV
Composition-based energy adjustment (-0.503 eV/atom x 4.0 atoms) = -2.0120 eV
Composition-based energy adjustment (-0.422 eV/atom x 4.0 atoms) = -1.6880 eV
Corrected energy = -87.5232 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)