material

BaCN2

ID:

mp-1029375


Tags: CNGMD Nitrides

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.983 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.53 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.953 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <0 0 1> <0 0 1> 0.000 114.2
KCl (mp-23193) <1 1 1> <0 0 1> 0.001 212.1
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.002 212.1
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.003 65.3
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.003 212.1
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.004 114.2
WS2 (mp-224) <0 0 1> <0 0 1> 0.004 114.2
WSe2 (mp-1821) <1 1 0> <0 0 1> 0.007 261.1
ZnO (mp-2133) <0 0 1> <0 0 1> 0.008 65.3
BN (mp-984) <0 0 1> <0 0 1> 0.009 16.3
C (mp-48) <0 0 1> <0 0 1> 0.009 146.8
MoSe2 (mp-1634) <1 1 1> <1 0 0> 0.009 268.8
BN (mp-984) <1 0 0> <1 1 0> 0.009 116.4
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.011 195.8
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.012 212.1
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.021 195.8
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.025 261.1
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.026 244.7
CaCO3 (mp-3953) <1 0 0> <0 0 1> 0.027 261.1
BN (mp-984) <1 0 1> <0 0 1> 0.028 179.5
TePb (mp-19717) <1 0 0> <0 0 1> 0.028 342.6
Ga2O3 (mp-886) <1 0 1> <1 1 0> 0.028 232.8
GaP (mp-2490) <1 1 1> <0 0 1> 0.030 212.1
ZnO (mp-2133) <1 0 1> <0 0 1> 0.031 277.4
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.033 195.8
Al (mp-134) <1 1 1> <0 0 1> 0.035 114.2
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.036 277.4
Cu (mp-30) <1 0 0> <1 0 1> 0.039 207.5
SiC (mp-7631) <1 0 0> <1 1 0> 0.042 232.8
LiF (mp-1138) <1 1 1> <0 0 1> 0.043 114.2
Ni (mp-23) <1 0 0> <0 0 1> 0.045 261.1
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.046 359.0
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.047 195.8
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.049 342.6
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.050 114.2
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.051 326.3
Ni (mp-23) <1 1 0> <0 0 1> 0.052 261.1
GaAs (mp-2534) <1 1 0> <0 0 1> 0.055 326.3
TePb (mp-19717) <1 1 0> <0 0 1> 0.056 244.7
TiO2 (mp-390) <1 0 0> <0 0 1> 0.059 146.8
BN (mp-984) <1 1 1> <1 0 0> 0.060 67.2
InAs (mp-20305) <1 1 1> <0 0 1> 0.064 65.3
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.067 114.2
AlN (mp-661) <1 0 0> <1 1 0> 0.070 232.8
Ge (mp-32) <1 1 0> <0 0 1> 0.071 326.3
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.074 65.3
ZrO2 (mp-2858) <1 1 -1> <0 0 1> 0.076 228.4
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.079 116.4
MoSe2 (mp-1634) <1 0 1> <0 0 1> 0.080 310.0
C (mp-66) <1 0 0> <1 0 1> 0.081 207.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
68 30 37 -2 0 0
30 68 37 2 0 0
37 37 92 0 0 0
-2 2 0 4 0 0
0 0 0 0 4 -2
0 0 0 0 -2 19
Compliance Tensor Sij (10-12Pa-1)
21.1 -6.7 -5.7 14.1 0 0
-6.7 21.1 -5.7 -14.1 0 0
-5.7 -5.7 15.5 0 0 0
14.1 -14.1 0 241.7 0 0
0 0 0 0 241.7 28.2
0 0 0 0 28.2 55.7
Shear Modulus GV
14 GPa
Bulk Modulus KV
48 GPa
Shear Modulus GR
8 GPa
Bulk Modulus KR
47 GPa
Shear Modulus GVRH
11 GPa
Bulk Modulus KVRH
48 GPa
Elastic Anisotropy
3.95
Poisson's Ratio
0.39

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.72 -0.00 0.00
-0.00 2.72 0.00
0.00 0.00 4.27
Dielectric Tensor εij (total)
8.60 -0.00 0.00
-0.00 8.60 0.00
0.00 0.00 11.75
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.24
Polycrystalline dielectric constant εpoly
(total)
9.65
Refractive Index n
1.80
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
DyHO2 (mp-755252) 0.2169 0.073 3
HoHO2 (mp-755716) 0.2222 0.084 3
YHO2 (mp-768231) 0.2135 0.081 3
NaHF2 (mp-27837) 0.2487 0.000 3
SrCN2 (mp-12317) 0.1543 0.000 3
KC2IN2 (mp-567299) 0.5359 0.467 4
NaCNO (mp-546500) 0.4550 0.000 4
NaAg(CN)2 (mp-568422) 0.4861 0.219 4
KAg(CN)2 (mp-582994) 0.5432 0.193 4
KAu(CN)2 (mp-672348) 0.4783 0.121 4
NaN3 (mp-22003) 0.5106 0.000 2
NaN3 (mp-570538) 0.5508 0.002 2
NaN3 (mp-1066400) 0.3337 0.002 2
LiN3 (mp-2659) 0.5389 0.000 2
LiEu4C3(IN2)3 (mp-638276) 0.7306 0.000 5
K2NaAg3(CN)6 (mp-6855) 0.7082 0.209 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv C N
Final Energy/Atom
-7.7472 eV
Corrected Energy
-30.9887 eV
-30.9887 eV = -30.9887 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • CNGMD Nitrides

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)