material

Mg2NbN3

ID:

mp-1029408


Tags: CNGMD Nitrides

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.147 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.031 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.75 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Mg2NbN3
Band Gap
2.516 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmc21 [36]
Hall
C 2c 2
Point Group
mm2
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.001 61.3
Mg (mp-153) <1 0 1> <1 1 0> 0.004 188.4
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.005 324.6
CdWO4 (mp-19387) <1 0 1> <0 1 0> 0.008 223.0
ZnO (mp-2133) <1 0 1> <0 1 1> 0.011 138.1
MgO (mp-1265) <1 1 0> <0 1 0> 0.015 127.4
Cu (mp-30) <1 1 0> <0 0 1> 0.026 183.8
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.030 108.2
SiC (mp-11714) <1 1 1> <1 0 1> 0.038 163.4
SiC (mp-11714) <1 1 0> <1 0 0> 0.045 54.1
LiNbO3 (mp-3731) <1 0 0> <0 1 0> 0.074 223.0
Fe3O4 (mp-19306) <1 1 1> <0 1 0> 0.076 127.4
MoSe2 (mp-1634) <1 0 1> <1 1 1> 0.078 263.1
YAlO3 (mp-3792) <1 0 0> <0 1 0> 0.078 159.3
LiNbO3 (mp-3731) <0 0 1> <0 1 0> 0.084 95.6
Al (mp-134) <1 0 0> <0 0 1> 0.087 245.0
C (mp-66) <1 0 0> <0 0 1> 0.088 306.3
KCl (mp-23193) <1 1 1> <0 1 0> 0.089 286.8
TiO2 (mp-2657) <1 0 0> <0 1 0> 0.089 223.0
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.103 245.0
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.113 183.8
BN (mp-984) <1 0 1> <1 0 0> 0.137 162.3
LaAlO3 (mp-2920) <0 0 1> <0 1 0> 0.139 350.5
LiTaO3 (mp-3666) <0 0 1> <0 1 0> 0.154 95.6
NdGaO3 (mp-3196) <1 1 1> <1 0 0> 0.160 270.5
CdS (mp-672) <1 1 1> <1 1 0> 0.166 313.9
CdS (mp-672) <1 0 0> <0 1 0> 0.172 254.9
ZnO (mp-2133) <1 0 0> <0 1 0> 0.174 159.3
C (mp-66) <1 1 1> <1 0 0> 0.176 270.5
C (mp-66) <1 1 0> <0 0 1> 0.176 183.8
CdWO4 (mp-19387) <1 0 0> <0 1 0> 0.185 31.9
CaCO3 (mp-3953) <0 0 1> <1 0 0> 0.198 270.5
C (mp-48) <0 0 1> <1 0 0> 0.200 270.5
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.201 188.4
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.205 216.4
MgO (mp-1265) <1 0 0> <0 0 1> 0.208 183.8
PbS (mp-21276) <1 1 0> <0 1 1> 0.209 207.1
Te2W (mp-22693) <0 0 1> <1 0 0> 0.209 270.5
Cu (mp-30) <1 1 1> <0 0 1> 0.215 183.8
TiO2 (mp-2657) <1 1 0> <0 1 0> 0.216 159.3
AlN (mp-661) <1 1 0> <1 0 0> 0.216 54.1
GaTe (mp-542812) <1 1 0> <0 1 0> 0.229 191.2
YAlO3 (mp-3792) <0 1 1> <0 1 0> 0.233 95.6
KTaO3 (mp-3614) <1 1 0> <0 1 0> 0.239 159.3
Ga2O3 (mp-886) <1 0 0> <0 1 0> 0.242 127.4
Ni (mp-23) <1 1 0> <0 1 0> 0.246 159.3
ZrO2 (mp-2858) <1 0 1> <0 1 0> 0.247 127.4
GaTe (mp-542812) <0 0 1> <0 1 0> 0.248 223.0
Ga2O3 (mp-886) <0 1 0> <0 1 0> 0.250 286.8
AlN (mp-661) <1 1 1> <0 1 0> 0.250 223.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
209 90 103 0 0 0
90 210 89 0 0 0
103 89 126 0 0 0
0 0 0 64 0 0
0 0 0 0 65 0
0 0 0 0 0 49
Compliance Tensor Sij (10-12Pa-1)
8.2 -0.9 -6 0 0 0
-0.9 6.9 -4.2 0 0 0
-6 -4.2 15.8 0 0 0
0 0 0 15.7 0 0
0 0 0 0 15.4 0
0 0 0 0 0 20.5
Shear Modulus GV
53 GPa
Bulk Modulus KV
123 GPa
Shear Modulus GR
46 GPa
Bulk Modulus KR
115 GPa
Shear Modulus GVRH
50 GPa
Bulk Modulus KVRH
119 GPa
Elastic Anisotropy
0.78
Poisson's Ratio
0.32

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 0.18332 0.00000
0.00000 0.00000 0.00000 0.14197 0.00000 0.00000
0.44967 0.36623 -1.46256 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
1.57334 C/m2
Crystallographic Direction vmax
0.00000
1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.44 0.00 0.00
0.00 5.65 0.00
0.00 0.00 6.00
Dielectric Tensor εij (total)
9.85 0.00 0.00
0.00 10.39 0.00
0.00 0.00 12.59
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.70
Polycrystalline dielectric constant εpoly
(total)
10.94
Refractive Index n
2.39
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiGaO2 (mp-5854) 0.2647 0.000 3
Li2CrO3 (mp-770149) 0.2238 0.072 3
TiZnN2 (mp-1016108) 0.2611 0.000 3
Mg2TaN3 (mp-1029442) 0.0701 0.000 3
Mg2SbN3 (mp-1029378) 0.2154 0.000 3
Li4MnV3O8 (mp-771529) 0.1514 0.108 4
Li2AlVO4 (mp-770519) 0.1778 0.091 4
Li4VFe3O8 (mp-773243) 0.1618 0.083 4
Li2AlVO4 (mp-769765) 0.1659 0.089 4
LiMn7O7F (mp-764671) 0.1798 0.083 4
PrH (mp-975657) 0.2614 0.082 2
PmH (mp-863656) 0.2723 0.000 2
CdO (mp-13119) 0.3140 0.007 2
ZrN (mp-13126) 0.3102 0.448 2
AcN (mp-866056) 0.3043 0.000 2
Ge (mp-1007760) 0.5205 0.022 1
Si (mp-165) 0.5246 0.013 1
C (mp-47) 0.5280 0.162 1
C (mp-1078845) 0.5068 0.266 1
C (mp-1080826) 0.5525 0.299 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Nb_pv N
Final Energy/Atom
-7.3399 eV
Corrected Energy
-88.0794 eV
-88.0794 eV = -88.0794 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • CNGMD Nitrides

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)