material

Ca3MoN3

ID:

mp-1029719


Tags: CNGMD Nitrides

Material Details

Final Magnetic Moment
0.831 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.993 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.45 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/m [176]
Hall
-P 6c
Point Group
6/m
Crystal System
hexagonal
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.000 153.1
Mg (mp-153) <0 0 1> <0 0 1> 0.001 341.7
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.011 195.3
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.013 341.7
WS2 (mp-224) <0 0 1> <0 0 1> 0.013 341.7
ZnO (mp-2133) <0 0 1> <0 0 1> 0.020 195.3
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.020 66.3
BN (mp-984) <0 0 1> <0 0 1> 0.021 48.8
TePb (mp-19717) <1 1 0> <0 0 1> 0.021 244.1
C (mp-48) <0 0 1> <0 0 1> 0.022 146.5
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.025 195.3
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.027 195.3
BN (mp-984) <1 1 1> <1 0 0> 0.027 306.1
WS2 (mp-224) <1 0 1> <1 0 0> 0.033 229.6
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.034 267.9
TePb (mp-19717) <1 0 0> <0 0 1> 0.036 341.7
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.043 229.6
C (mp-66) <1 1 0> <1 1 0> 0.047 198.8
TiO2 (mp-390) <1 0 0> <0 0 1> 0.057 146.5
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.057 195.3
Al (mp-134) <1 1 1> <0 0 1> 0.057 195.3
ZrO2 (mp-2858) <1 1 -1> <1 0 0> 0.059 229.6
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.065 341.7
TiO2 (mp-390) <0 0 1> <1 0 0> 0.071 114.8
BN (mp-984) <1 0 1> <1 1 0> 0.075 265.1
CaCO3 (mp-3953) <1 0 0> <1 1 0> 0.075 265.1
KCl (mp-23193) <1 0 0> <0 0 1> 0.089 244.1
MoS2 (mp-1434) <1 0 0> <1 0 0> 0.093 267.9
InAs (mp-20305) <1 1 1> <0 0 1> 0.097 195.3
AlN (mp-661) <1 0 1> <0 0 1> 0.100 195.3
LiTaO3 (mp-3666) <0 0 1> <1 0 1> 0.104 186.1
MgO (mp-1265) <1 0 0> <1 1 1> 0.105 164.6
GaSe (mp-1943) <1 0 0> <1 0 0> 0.105 267.9
GaSe (mp-1943) <0 0 1> <1 1 0> 0.108 198.8
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.111 195.3
ZnO (mp-2133) <1 1 1> <1 0 0> 0.112 191.3
ZrO2 (mp-2858) <1 0 1> <0 0 1> 0.112 341.7
ZnSe (mp-1190) <1 0 0> <1 1 1> 0.112 164.6
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.117 306.1
Au (mp-81) <1 1 1> <1 0 0> 0.117 153.1
LiGaO2 (mp-5854) <1 1 0> <1 0 0> 0.117 191.3
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.121 244.1
Ni (mp-23) <1 1 1> <0 0 1> 0.122 146.5
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.124 195.3
GaAs (mp-2534) <1 0 0> <1 1 1> 0.128 164.6
GaN (mp-804) <1 0 1> <0 0 1> 0.130 244.1
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.130 191.3
C (mp-66) <1 1 1> <0 0 1> 0.139 195.3
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.140 344.4
CdTe (mp-406) <1 1 0> <0 0 1> 0.140 244.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
73 53 33 0 0 0
53 73 33 0 0 0
33 33 127 0 0 0
0 0 0 40 0 0
0 0 0 0 40 0
0 0 0 0 0 10
Compliance Tensor Sij (10-12Pa-1)
29.7 -20.4 -2.4 0 0 0
-20.4 29.7 -2.4 0 0 0
-2.4 -2.4 9.1 0 0 0
0 0 0 25 0 0
0 0 0 0 25 0
0 0 0 0 0 100.1
Shear Modulus GV
28 GPa
Bulk Modulus KV
57 GPa
Shear Modulus GR
18 GPa
Bulk Modulus KR
56 GPa
Shear Modulus GVRH
23 GPa
Bulk Modulus KVRH
56 GPa
Elastic Anisotropy
2.77
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ca3MoN3 (mp-1080844) 0.0200 0.000 3
Na3CoO3 (mp-776646) 0.6276 0.144 3
Sr3WN3 (mp-1029655) 0.5140 0.000 3
Ba3CrN3 (mp-12905) 0.5973 0.000 3
Sr3BN3 (mp-1029665) 0.5804 0.087 3
LiFeBO3 (mp-779311) 0.6467 0.054 4
LiMnBO3 (mp-769939) 0.6173 0.094 4
LiFeBO3 (mp-769690) 0.5279 0.084 4
Li3Cr(BO3)2 (mp-769732) 0.6282 0.054 4
Ba4GaN3O (mp-1019516) 0.6357 0.064 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Mo_pv N
Final Energy/Atom
-6.8077 eV
Corrected Energy
-95.3085 eV
-95.3085 eV = -95.3085 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • CNGMD Nitrides

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)