material

SbPt7

ID:

mp-1030

DOI:

10.17188/1186885


Tags: Platinum antimonide (7/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.108 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.007 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
18.87 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Sb2Pt3 + Pt
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 54340 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.000 65.0
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.000 91.9
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.000 112.5
ZnO (mp-2133) <0 0 1> <1 1 1> 0.001 112.5
PbS (mp-21276) <1 0 0> <1 0 0> 0.002 324.8
NaCl (mp-22862) <1 0 0> <1 0 0> 0.008 65.0
NaCl (mp-22862) <1 1 0> <1 1 0> 0.008 91.9
C (mp-48) <1 0 1> <1 0 0> 0.009 259.9
TiO2 (mp-390) <0 0 1> <1 0 0> 0.013 129.9
SiC (mp-8062) <1 0 0> <1 0 0> 0.016 324.8
MgO (mp-1265) <1 0 0> <1 0 0> 0.017 324.8
Al (mp-134) <1 0 0> <1 0 0> 0.021 65.0
Al (mp-134) <1 1 0> <1 1 0> 0.022 91.9
Al (mp-134) <1 1 1> <1 1 1> 0.022 112.5
TePb (mp-19717) <1 1 0> <1 1 0> 0.023 183.8
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.031 259.9
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.039 91.9
Cu (mp-30) <1 0 0> <1 0 0> 0.047 65.0
KCl (mp-23193) <1 0 0> <1 0 0> 0.059 324.8
AlN (mp-661) <1 0 1> <1 0 0> 0.060 194.9
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.067 91.9
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.072 183.8
CdS (mp-672) <1 1 1> <1 0 0> 0.074 259.9
DyScO3 (mp-31120) <0 1 0> <1 0 0> 0.094 129.9
GaSe (mp-1943) <0 0 1> <1 1 1> 0.104 112.5
BN (mp-984) <1 0 0> <1 0 0> 0.114 194.9
Ni (mp-23) <1 1 0> <1 1 0> 0.121 275.6
ZrO2 (mp-2858) <1 0 1> <1 0 0> 0.140 129.9
TeO2 (mp-2125) <0 1 0> <1 1 0> 0.151 275.6
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.165 65.0
ZnO (mp-2133) <1 0 0> <1 0 0> 0.169 259.9
SiC (mp-7631) <0 0 1> <1 0 0> 0.179 324.8
SiC (mp-11714) <0 0 1> <1 0 0> 0.184 324.8
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.192 194.9
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.202 259.9
TbScO3 (mp-31119) <0 1 0> <1 0 0> 0.203 129.9
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.204 91.9
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.213 65.0
NdGaO3 (mp-3196) <1 0 1> <1 0 0> 0.219 324.8
Mg (mp-153) <1 1 0> <1 0 0> 0.239 259.9
BN (mp-984) <1 0 1> <1 1 0> 0.242 183.8
CdTe (mp-406) <1 1 0> <1 1 0> 0.244 183.8
Ni (mp-23) <1 0 0> <1 0 0> 0.248 324.8
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.250 129.9
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.253 65.0
Mg (mp-153) <1 0 0> <1 1 0> 0.255 183.8
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.261 91.9
InSb (mp-20012) <1 1 0> <1 1 0> 0.289 183.8
C (mp-66) <1 0 0> <1 0 0> 0.304 65.0
LiF (mp-1138) <1 1 0> <1 0 0> 0.306 324.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
234 198 198 0 0 0
198 234 198 0 0 0
198 198 234 0 0 0
0 0 0 47 0 0
0 0 0 0 47 0
0 0 0 0 0 47
Compliance Tensor Sij (10-12Pa-1)
19.1 -8.8 -8.8 0 0 0
-8.8 19.1 -8.8 0 0 0
-8.8 -8.8 19.1 0 0 0
0 0 0 21.1 0 0
0 0 0 0 21.1 0
0 0 0 0 0 21.1
Shear Modulus GV
36 GPa
Bulk Modulus KV
210 GPa
Shear Modulus GR
29 GPa
Bulk Modulus KR
210 GPa
Shear Modulus GVRH
32 GPa
Bulk Modulus KVRH
210 GPa
Elastic Anisotropy
1.23
Poisson's Ratio
0.43

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1125 0.003 3
CrCoPt2 (mp-570863) 0.0492 0.036 3
LiCa6Ge (mp-12609) 0.0000 0.185 3
GaFeNi2 (mp-1065359) 0.0412 0.067 3
GaCo2Ni (mp-1018060) 0.0157 0.079 3
Cr8Ni50Mo15W2 (mp-767372) 0.2155 0.028 4
CrFeCoNi (mp-1012640) 0.3608 0.057 4
CrFeCoNi (mp-1096923) 0.4019 0.129 4
Ti3Ni (mp-981209) 0.0000 0.127 2
Mg3Mo (mp-978287) 0.0000 0.321 2
CuPt7 (mp-12608) 0.0000 0.000 2
LiPt7 (mp-30765) 0.0000 0.000 2
Ca7Ge (mp-10008) 0.0000 0.222 2
Hf (mp-8640) 0.0000 0.071 1
Pa (mp-10740) 0.0000 0.000 1
Ag (mp-124) 0.0000 0.002 1
Zr (mp-8635) 0.0000 0.041 1
Er (mp-10752) 0.0000 0.028 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sb Pt
Final Energy/Atom
-5.9236 eV
Corrected Energy
-47.3887 eV
-47.3887 eV = -47.3887 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 57471
  • 54340
Submitted by
User remarks:
  • Platinum antimonide (7/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)