Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.477 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.140 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + Te2W + WS2 + MoWSe4 |
Band Gap0.301 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 70.2 |
C (mp-48) | <1 0 0> | <0 0 1> | 250.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 291.0 |
C (mp-48) | <1 1 0> | <0 0 1> | 240.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 311.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 130.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 250.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 190.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 190.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 170.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 321.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 351.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 160.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 100.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 140.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 351.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 281.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 70.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 90.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 190.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 281.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 70.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 160.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 331.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 140.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 281.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 351.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 271.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 70.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 100.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 140.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 180.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 200.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 190.7 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 180.6 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 190.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 230.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 160.6 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 281.0 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 281.0 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 250.9 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 250.9 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 130.5 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 220.8 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 250.9 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 311.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 351.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 311.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 130.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 281.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeMoS (mp-1027412) | 0.1198 | 0.078 | 3 |
Te3W2S (mp-1028755) | 0.1106 | 0.083 | 3 |
TeWS (mp-1028690) | 0.1151 | 0.097 | 3 |
Te4W3S2 (mp-1026362) | 0.1276 | 0.092 | 3 |
TeWS (mp-1028526) | 0.1241 | 0.097 | 3 |
Te2W2SeS (mp-1028732) | 0.0497 | 0.074 | 4 |
Te2Mo2SeS (mp-1026983) | 0.0464 | 0.058 | 4 |
TeMo2Se2S (mp-1026958) | 0.0858 | 0.040 | 4 |
Te2W2SeS (mp-1028445) | 0.0630 | 0.072 | 4 |
Te2Mo2SeS (mp-1030775) | 0.0651 | 0.056 | 4 |
WSe2 (mp-1028698) | 0.3460 | 0.000 | 2 |
WS2 (mp-1028441) | 0.3417 | 0.001 | 2 |
MoSe2 (mp-1027692) | 0.3461 | 0.000 | 2 |
WSe2 (mp-1025572) | 0.3460 | 0.000 | 2 |
WS2 (mp-1025571) | 0.3434 | 0.001 | 2 |
Te4MoW3(SeS)2 (mp-1030159) | 0.0502 | 0.090 | 5 |
Te4MoW3(SeS)2 (mp-1028689) | 0.0516 | 0.092 | 5 |
Te4Mo3W(SeS)2 (mp-1026972) | 0.0471 | 0.118 | 5 |
Te4MoW3(SeS)2 (mp-1028510) | 0.0479 | 0.127 | 5 |
Te2MoWSeS (mp-1027736) | 0.0463 | 0.140 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv Se S |
Final Energy/Atom-6.6537 eV |
Corrected Energy-83.4818 eV
Uncorrected energy = -79.8438 eV
Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV
Composition-based energy adjustment (-0.472 eV/atom x 2.0 atoms) = -0.9440 eV
Composition-based energy adjustment (-0.422 eV/atom x 4.0 atoms) = -1.6880 eV
Corrected energy = -83.4818 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)