Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.523 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.084 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + MoSe2 + MoWSe4 |
Band Gap0.515 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 69.3 |
C (mp-48) | <1 0 0> | <0 0 1> | 247.5 |
C (mp-48) | <1 0 1> | <0 0 1> | 287.1 |
C (mp-48) | <1 1 0> | <0 0 1> | 237.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 188.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 128.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 247.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 237.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 247.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 168.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 346.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 158.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 99.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 237.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 277.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 69.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 69.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 247.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 247.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 207.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 69.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 158.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 138.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 277.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 346.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 267.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 69.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 99.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 138.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 49.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 118.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.7 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 178.2 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 188.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 158.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 277.2 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 247.5 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 247.5 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 247.5 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 128.7 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 217.8 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 247.5 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 306.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 316.8 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 316.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 306.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 128.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 277.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 267.3 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 237.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeW2Se3 (mp-1028731) | 0.0224 | 0.029 | 3 |
Te2W3Se4 (mp-1026348) | 0.0312 | 0.036 | 3 |
Te2Mo3Se4 (mp-1025876) | 0.0425 | 0.025 | 3 |
TeMo2Se3 (mp-1027818) | 0.0058 | 0.022 | 3 |
TeMo2Se3 (mp-1027682) | 0.0754 | 0.022 | 3 |
TeMoWSe3 (mp-1030466) | 0.0076 | 0.109 | 4 |
Te2Mo3WSe6 (mp-1030410) | 0.0072 | 0.084 | 4 |
TeMoWSe3 (mp-1029243) | 0.0075 | 0.109 | 4 |
TeMoWSe3 (mp-1029165) | 0.0103 | 0.108 | 4 |
Te2Mo3WSe6 (mp-1028419) | 0.0029 | 0.084 | 4 |
WSe2 (mp-1028698) | 0.1913 | 0.000 | 2 |
MoSe2 (mp-1025799) | 0.2004 | 0.000 | 2 |
MoSe2 (mp-1027692) | 0.1979 | 0.000 | 2 |
WSe2 (mp-1025572) | 0.1935 | 0.000 | 2 |
WSe2 (mp-1023933) | 0.2026 | 0.001 | 2 |
TeMoWSe2S (mp-1028948) | 0.1524 | 0.104 | 5 |
Te2MoW3(Se2S)2 (mp-1028850) | 0.1475 | 0.111 | 5 |
Te2MoW3(Se2S)2 (mp-1028709) | 0.1521 | 0.090 | 5 |
Te2Mo3W(Se2S)2 (mp-1027721) | 0.1512 | 0.086 | 5 |
TeMoWSe2S (mp-1080189) | 0.1529 | 0.104 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv Se |
Final Energy/Atom-6.5860 eV |
Corrected Energy-82.7082 eV
Uncorrected energy = -79.0322 eV
Composition-based energy adjustment (-0.472 eV/atom x 6.0 atoms) = -2.8320 eV
Composition-based energy adjustment (-0.422 eV/atom x 2.0 atoms) = -0.8440 eV
Corrected energy = -82.7082 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)