Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.445 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.029 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + MoSe2 |
Band Gap0.746 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [164] |
Hall-P 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 71.8 |
C (mp-48) | <1 0 0> | <0 0 1> | 256.3 |
C (mp-48) | <1 0 1> | <0 0 1> | 338.3 |
C (mp-48) | <1 1 0> | <0 0 1> | 317.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 71.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 133.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 256.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 276.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 174.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 235.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 164.0 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 164.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 358.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 276.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 71.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 92.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 194.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 276.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 287.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 71.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 287.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 338.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 194.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 164.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 184.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 205.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 194.8 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 246.1 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 246.1 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 194.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 134.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 164.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 287.1 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 266.6 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 317.8 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 256.3 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 225.5 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 235.8 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 317.8 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 215.3 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 71.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 133.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 287.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 276.8 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 287.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 61.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 123.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 194.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 71.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeWSe (mp-1028749) | 0.0624 | 0.043 | 3 |
Te4W3Se2 (mp-1026350) | 0.0622 | 0.044 | 3 |
TeWSe (mp-1028459) | 0.0207 | 0.043 | 3 |
Te2Mo3Se4 (mp-1025728) | 0.0614 | 0.025 | 3 |
TeMoSe (mp-1027683) | 0.0550 | 0.029 | 3 |
Te4Mo3WSe4 (mp-1030616) | 0.0094 | 0.111 | 4 |
Te4Mo3WSe4 (mp-1030573) | 0.0080 | 0.091 | 4 |
Te2MoWSe2 (mp-1030239) | 0.0118 | 0.098 | 4 |
Te2MoWSe2 (mp-1029066) | 0.0119 | 0.118 | 4 |
Te2MoWSe2 (mp-1030695) | 0.0121 | 0.098 | 4 |
Te2Mo (mp-1030319) | 0.2259 | 0.000 | 2 |
Te2W (mp-1028586) | 0.2244 | 0.025 | 2 |
Te2Mo (mp-1025576) | 0.2278 | 0.000 | 2 |
Te2W (mp-1025573) | 0.2270 | 0.026 | 2 |
Te2W (mp-1023942) | 0.2318 | 0.026 | 2 |
TeMoWSe2S (mp-1030162) | 0.1303 | 0.125 | 5 |
TeMoWSe2S (mp-1029116) | 0.1282 | 0.104 | 5 |
TeMoWSe2S (mp-1027138) | 0.1270 | 0.120 | 5 |
Te2Mo3W(Se2S)2 (mp-1027137) | 0.1288 | 0.103 | 5 |
Te2Mo3W(Se2S)2 (mp-1030827) | 0.1232 | 0.087 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv Se |
Final Energy/Atom-6.2738 eV |
Corrected Energy-75.2853 eV
-75.2853 eV = -75.2853 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)