Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.473 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.129 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe2Mo + Te2W + MoWSe4 |
Band Gap0.582 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 69.4 |
C (mp-48) | <1 0 0> | <0 0 1> | 247.8 |
C (mp-48) | <1 0 1> | <0 0 1> | 287.5 |
C (mp-48) | <1 1 0> | <0 0 1> | 237.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 188.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 128.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 247.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 237.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 247.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 168.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 346.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 158.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 99.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 237.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 277.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 69.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 69.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 247.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 247.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 208.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 69.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 158.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 138.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 277.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 346.9 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 267.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 69.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 99.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 138.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 49.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 119.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.7 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 178.4 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 188.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 158.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 277.6 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 247.8 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 247.8 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 247.8 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 128.9 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 218.1 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 247.8 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 307.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 317.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 317.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 307.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 128.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 277.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 267.6 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 237.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TeW2Se3 (mp-1028762) | 0.0143 | 0.030 | 3 |
Te2W3Se4 (mp-1026349) | 0.0317 | 0.036 | 3 |
TeWSe (mp-1028459) | 0.0727 | 0.043 | 3 |
Te2Mo3Se4 (mp-1025728) | 0.0478 | 0.025 | 3 |
TeMo2Se3 (mp-1027682) | 0.0090 | 0.022 | 3 |
TeMoWSe3 (mp-1030509) | 0.0030 | 0.129 | 4 |
Te2Mo3WSe6 (mp-1030605) | 0.0081 | 0.084 | 4 |
TeMoWSe3 (mp-1030163) | 0.0028 | 0.129 | 4 |
Te2Mo(WSe2)3 (mp-1029073) | 0.0055 | 0.091 | 4 |
Te2Mo(WSe2)3 (mp-1028848) | 0.0097 | 0.091 | 4 |
Te2Mo (mp-1030319) | 0.1975 | 0.000 | 2 |
Te2W (mp-1028586) | 0.1955 | 0.025 | 2 |
Te2Mo (mp-1025576) | 0.1983 | 0.000 | 2 |
Te2W (mp-1025573) | 0.1963 | 0.026 | 2 |
Te2W (mp-1023942) | 0.2006 | 0.026 | 2 |
TeMoWSe2S (mp-1030578) | 0.1533 | 0.104 | 5 |
Te2Mo3W(Se2S)2 (mp-1030575) | 0.1533 | 0.087 | 5 |
TeMoWSe2S (mp-1030515) | 0.1534 | 0.104 | 5 |
Te2MoW3(Se2S)2 (mp-1029078) | 0.1571 | 0.111 | 5 |
TeMoWSe2S (mp-1080236) | 0.1579 | 0.125 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Mo_pv W_pv Se |
Final Energy/Atom-6.7125 eV |
Corrected Energy-80.5502 eV
-80.5502 eV = -80.5502 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)