Final Magnetic Moment0.012 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.773 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 315.7 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 315.7 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 245.6 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 312.9 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 108.4 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 189.4 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 312.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 126.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 189.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 260.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 312.9 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 252.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 123.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 189.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 189.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 63.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 260.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 108.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 189.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 312.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 189.4 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 260.7 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 260.7 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 246.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 312.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 189.4 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 156.4 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 245.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 189.4 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 189.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 252.5 |
BN (mp-984) | <1 0 0> | <1 0 0> | 315.7 |
BN (mp-984) | <1 0 1> | <1 0 0> | 315.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 260.7 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 312.9 |
Al (mp-134) | <1 0 0> | <0 1 0> | 312.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 189.4 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 252.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 252.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 315.7 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 63.1 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 315.7 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 315.7 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 315.7 |
SiC (mp-7631) | <1 0 1> | <1 1 -1> | 240.5 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 252.5 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 208.6 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 126.3 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 260.7 |
C (mp-66) | <1 1 0> | <0 1 0> | 260.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y2Si5Rh3 (mp-9882) | 0.2135 | 0.000 | 3 |
Ho2Ge5Rh3 (mp-17534) | 0.2772 | 0.000 | 3 |
Tb2Si5Rh3 (mp-12879) | 0.2147 | 0.000 | 3 |
Lu2Co3Si5 (mp-15826) | 0.1461 | 0.000 | 3 |
Dy2Co3Si5 (mp-15898) | 0.0376 | 0.000 | 3 |
KNa4SnSb3 (mp-6758) | 0.7483 | 0.005 | 4 |
V3S4 (mp-560908) | 0.6406 | 0.253 | 2 |
Mg2Si3 (mp-1073037) | 0.6129 | 0.180 | 2 |
MgSi2 (mp-1073454) | 0.6229 | 0.195 | 2 |
MgSi (mp-1073686) | 0.6445 | 0.165 | 2 |
Mg3Si4 (mp-1075157) | 0.6544 | 0.187 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Co Si |
Final Energy/Atom-6.5439 eV |
Corrected Energy-130.1678 eV
Uncorrected energy = -130.8778 eV
Composition-based energy adjustment (0.071 eV/atom x 10.0 atoms) = 0.7100 eV
Corrected energy = -130.1678 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)