Final Magnetic Moment0.269 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.004 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.130 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa5Zn3 + Ca |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 0 0> | 128.7 |
C (mp-48) | <1 0 0> | <1 0 0> | 77.2 |
C (mp-48) | <1 0 1> | <1 1 0> | 291.3 |
C (mp-48) | <1 1 0> | <1 1 0> | 327.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 178.4 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 133.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 77.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 231.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 109.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 231.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 327.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 128.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 145.6 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 178.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 206.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 109.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 128.7 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 109.2 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 283.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 109.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 206.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 109.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 291.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 128.7 |
InAs (mp-20305) | <1 0 0> | <1 1 1> | 223.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 109.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 128.7 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 145.6 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 178.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 128.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 72.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 145.6 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 334.7 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 145.6 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 178.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 180.2 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 109.2 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 109.2 |
Te2W (mp-22693) | <1 1 1> | <1 1 1> | 223.0 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 154.5 |
CdWO4 (mp-19387) | <0 1 1> | <1 1 0> | 291.3 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 154.5 |
CdWO4 (mp-19387) | <1 1 0> | <1 1 0> | 291.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 206.0 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 312.2 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 44.6 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 109.2 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 223.0 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 206.0 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 180.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
30 | 30 | 30 | 0 | 0 | 0 |
30 | 30 | 30 | 0 | 0 | 0 |
30 | 30 | 30 | 0 | 0 | 0 |
0 | 0 | 0 | 16 | 0 | 0 |
0 | 0 | 0 | 0 | 16 | 0 |
0 | 0 | 0 | 0 | 0 | 16 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
28625 | -14306.9 | -14306.9 | 0 | 0 | 0 |
-14306.9 | 28625 | -14306.9 | 0 | 0 | 0 |
-14306.9 | -14306.9 | 28625 | 0 | 0 | 0 |
0 | 0 | 0 | 63.4 | 0 | 0 |
0 | 0 | 0 | 0 | 63.4 | 0 |
0 | 0 | 0 | 0 | 0 | 63.4 |
Shear Modulus GV9 GPa |
Bulk Modulus KV30 GPa |
Shear Modulus GR0 GPa |
Bulk Modulus KR30 GPa |
Shear Modulus GVRH5 GPa |
Bulk Modulus KVRH30 GPa |
Elastic Anisotropy1623.43 |
Poisson's Ratio0.42 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.034 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.183 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.065 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
Ge3Sb (mp-976111) | 0.0000 | 0.333 | 2 |
MnCo3 (mp-999563) | 0.0000 | 0.056 | 2 |
CrPt3 (mp-2515) | 0.0000 | 0.000 | 2 |
CaSn3 (mp-11290) | 0.0000 | 0.000 | 2 |
GdSn3 (mp-19919) | 0.0000 | 0.000 | 2 |
Sr (mp-76) | 0.0000 | 0.006 | 1 |
Mg (mp-1056702) | 0.0000 | 0.000 | 1 |
N2 (mp-1056857) | 0.0000 | 0.000 | 1 |
Ni (mp-1056486) | 0.0000 | 0.000 | 1 |
Cd (mp-1096861) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Zn |
Final Energy/Atom-1.8235 eV |
Corrected Energy-7.2941 eV
-7.2941 eV = -7.2941 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)