Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.014 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaMg2 + Ca |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 1 0> | 189.3 |
C (mp-48) | <1 0 1> | <1 0 0> | 256.8 |
C (mp-48) | <1 1 0> | <1 1 0> | 298.1 |
C (mp-48) | <1 1 1> | <0 1 0> | 302.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 207.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 283.3 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 236.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 189.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 265.1 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 298.1 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 340.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 265.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 189.3 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 78.9 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 113.6 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 265.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 321.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 94.4 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 151.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 207.8 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 113.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 64.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 207.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 189.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 113.6 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 223.6 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 321.0 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 149.1 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 113.6 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 302.9 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 207.8 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 0> | 149.1 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 321.0 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 277.0 |
CdWO4 (mp-19387) | <1 0 0> | <0 1 0> | 151.5 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 128.4 |
CdWO4 (mp-19387) | <1 1 0> | <0 1 0> | 340.8 |
CdWO4 (mp-19387) | <1 1 1> | <1 0 0> | 321.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 207.8 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 236.8 |
Ni (mp-23) | <1 0 0> | <0 1 1> | 157.9 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 151.5 |
Ni (mp-23) | <1 1 1> | <0 1 0> | 265.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 192.6 |
BN (mp-984) | <1 0 0> | <0 1 0> | 302.9 |
BN (mp-984) | <1 0 1> | <0 1 0> | 302.9 |
BN (mp-984) | <1 1 0> | <0 1 0> | 302.9 |
BN (mp-984) | <1 1 1> | <0 1 0> | 302.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 315.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 283.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiCuNi2 (mp-1079193) | 0.1318 | 0.021 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.3675 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.2123 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.3798 | 0.193 | 4 |
HfAu3 (mp-1079296) | 0.1048 | 0.000 | 2 |
Mg3Zn (mp-1094427) | 0.1234 | 0.071 | 2 |
Mg2Zn (mp-1094489) | 0.1299 | 0.083 | 2 |
Mg2Zn (mp-1094468) | 0.1184 | 0.061 | 2 |
Y (mp-1059189) | 0.2108 | 0.004 | 1 |
Er (mp-99) | 0.2200 | 0.007 | 1 |
Ho (mp-144) | 0.2201 | 0.010 | 1 |
Tm (mp-143) | 0.2234 | 0.004 | 1 |
Pr (mp-1009594) | 0.2206 | 0.032 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Mg_pv |
Final Energy/Atom-1.8849 eV |
Corrected Energy-11.3091 eV
-11.3091 eV = -11.3091 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)